Ultrasonic Flaw Detection at High Temperature SS piping weld joints

We intend to perform UFD on SS lines weld joints while in operation (temperature ~ 200 deg C). I need help in identification of hardware (probes), accessories and method of performing UFD on SS weld joints. Anybody having such experience may guide me. I will be grateful.


 
 Reply 
 
UT Roscomm
UT Roscomm
07:52 Jan-24-2008
Re: Ultrasonic Flaw Detection at High Temperature SS piping weld joints
----------- Start Original Message -----------
: We intend to perform UFD on SS lines weld joints while in operation (temperature ~ 200 deg C). I need help in identification of hardware (probes), accessories and method of performing UFD on SS weld joints. Anybody having such experience may guide me. I will be grateful.
------------ End Original Message ------------

You cannot do it with any reliability due the the interface between the weld and parent metal.


 
 Reply 
 
Collin Maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

Collin Maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
06:38 Feb-23-2008
Re: Ultrasonic Flaw Detection at High Temperature SS piping weld joints
----------- Start Original Message -----------
: : We intend to perform UFD on SS lines weld joints while in operation (temperature ~ 200 deg C). I need help in identification of hardware (probes), accessories and method of performing UFD on SS weld joints. Anybody having such experience may guide me. I will be grateful.
: You cannot do it with any reliability due the the interface between the weld and parent metal.
------------ End Original Message ------------

UFD of SS welds has been around for some time, see the IIW guide circa 1986. The testing at temperatures you are quoting, to my knowlege, is not possible. This is due to the probe design not able to withstand anything other than room temperature.



 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>