02:45 Jan-31-2000
Railways axis

Dear Friends:

I'd wish you to send me some information or recomendation about Ultrasonic and magnetic particles Testings applied to Railway-Axis inspection.

Best regards
Mario Belo



 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 182

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
182
02:16 Feb-01-2000
Re: Railways axis
reply by Udo Schlengermann
(uschlengermann@krautkramer.de)

Some information on ultrasonic testing of railway axles:
It makes a big difference
- wether you have to test new axles for internal defects
- or wether you have to make an inservice inspection looking for cracks.

For the second kind of inspection you need information on the axle type and shape, and where cracks are to be expected (under wheels or bearings,
or braking discs). It makes a difference wether axles are used on traction vehicles or on rolling wheelsets.
Most specifications for ultrasonic inservice inspection of axles are published by national railway companies.

For testing new axles there are a lot of internationally used specifications, e.g.

- ISO 1005-3
Railway rolling stock material - Axles for tractive and trailing stock - Quality requirements.

- ISO 5948
Railway rolling stock material - Ultrasonic acceptance testing.

- EN 13261 (draft)
Railways - Wheelsets and bogies - Axles - Product requirements.

- AAR
Manual of standards and recommended practices, (M10) chapter 18: Inspection

- ASTM A21
Standard specification for standard steel axles, non-heat treated and heat treated for railway use

Kind regards
Udo Schlengermann
++++++++++++++++

: Dear Friends:

: I'd wish you to send me some information or recomendation about Ultrasonic and magnetic particles Testings applied to Railway-Axis inspection.
:
: Best regards
: Mario Belo




 
 Reply 
 
Christoph Schnitger
Christoph Schnitger
09:32 Feb-02-2000
Re: Railways axis
Hello Mario,

some days ago i buy used equipment for ultrasonic testing of railways axis ( Krautkrämer probes with
test block for just.etc ).
Now i want to sell it, if you are interessted in buying the equipment,...no problem....at first please
contact me....i will sent some pics via Mail !

Do not hesitate to contact me !
C.Schnitger



 
 Reply 
 

Product Spotlight

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window