MRI on composites

I have been tasked to find an article or any information regarding Magnetic Resonance Imagery on composites, specifically focused on defect measurement. I have been trawling through google results for a while and cant seem to find anything relevant. If anyone out there can help or even give me a bit of advice it would really be appreciated.
Thanks in advance,
Chris Boyd


 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 304

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
304
09:53 Mar-07-2008
Re: MRI on composites
----------- Start Original Message -----------
: I have been tasked to find an article or any information regarding Magnetic Resonance Imagery on composites, specifically focused on defect measurement. I have been trawling through google results for a while and cant seem to find anything relevant. If anyone out there can help or even give me a bit of advice it would really be appreciated.
: Thanks in advance,
: Chris Boyd
------------ End Original Message ------------

Chris,
Is this a misunderstanding of terminology?
There are several "RESONANCE" applications within Composite inspection, but I have not come across MRI as a technique on composites. Could however be some applications there, so I would be interested if there are.

Godfrey Hands




 
 Reply 
 
Simon Amallraja
Simon Amallraja
07:05 Mar-07-2008
Re: MRI on composites
----------- Start Original Message -----------
: : I have been tasked to find an article or any information regarding Magnetic Resonance Imagery on composites, specifically focused on defect measurement. I have been trawling through google results for a while and cant seem to find anything relevant. If anyone out there can help or even give me a bit of advice it would really be appreciated.
: : Thanks in advance,
: : Chris Boyd
: Chris,
: Is this a misunderstanding of terminology?
: There are several "RESONANCE" applications within Composite inspection, but I have not come across MRI as a technique on composites. Could however be some applications there, so I would be interested if there are.
: Godfrey Hands
------------ End Original Message ------------

I think QNET, GmbH has One Side Access Magnetic Resonance Method Instrument for attenuating materials. Not specifically for Composites. Check up with them. www.qnet.com.

Simon Amallraja


 
 Reply 
 
Chris Boyd
Chris Boyd
03:48 Mar-09-2008
Re: MRI on composites
----------- Start Original Message -----------
: : : I have been tasked to find an article or any information regarding Magnetic Resonance Imagery on composites, specifically focused on defect measurement. I have been trawling through google results for a while and cant seem to find anything relevant. If anyone out there can help or even give me a bit of advice it would really be appreciated.
: : : Thanks in advance,
: : : Chris Boyd
: : Chris,
: : Is this a misunderstanding of terminology?
: : There are several "RESONANCE" applications within Composite inspection, but I have not come across MRI as a technique on composites. Could however be some applications there, so I would be interested if there are.
: : Godfrey Hands
: I think QNET, GmbH has One Side Access Magnetic Resonance Method Instrument for attenuating materials. Not specifically for Composites. Check up with them. www.qnet.com.
: Simon Amallraja
------------ End Original Message ------------

Thanks to Godfrey andSimon for your help. It sounds like relatively new technology and I'm only new to the game myself. I think that they're pulling the plug on it anyway.
Thank you for your help again.
Chris.



 
 Reply 
 
David Forsyth
R & D
TRI/Austin, USA, Joined Nov 2001, 41

David Forsyth

R & D
TRI/Austin,
USA,
Joined Nov 2001
41
09:36 Mar-11-2008
Re: MRI on composites
A few years ago, the University of New Brunswick (Canada) did some work using real MRI equipment on composite aircraft structure, go the this URL
http://www.unb.ca/fredericton/science/physics/mri/

And scroll down to year 2005. I do not know if this is still being funded.

Dave.


 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>