S.R.G.PRABHU
Consultant, AUT specialist
FREELANCE, India, Joined Aug 2008, 64

S.R.G.PRABHU

Consultant, AUT specialist
FREELANCE,
India,
Joined Aug 2008
64
01:39 Mar-30-2008
API-510 Pressure vessels inspection frequency

Hello,
I am working on a Gas gathering platform offshore. We need to know the frequency of the pressel vessels inspection, internal visual...As per API 510, what is the frequency of a vessel to be inspected which is 2 and half years old?Someone please advise.Is it once in 5 years?We have a shut down coming and planning has to be done.


 
 Reply 
 
Ryan Burns
Ryan Burns
02:00 Apr-01-2008
Re: API-510 Pressure vessels inspection frequency
See excerpt below. I would perform UT thickness to determine corrosion rate and establish appropriate frequency in accordance with applicable jurisdictional authority. If T/A timing allows, it would likely be advisable to conduct internal insp on inlet and any sour service vessels as a minimum in conjunction with a full corrosion survey of vessels and associated piping.

Good luck,

RB.

INTERNAL AND ON-STREAM INSPECTION
The period between internal or on-stream inspections shall
not exceed one half the estimated remaining life of the vessel
based on corrosion rate or 10 years, whichever is less. In
cases where the remaining safe operating life is estimated to
be less than 4 years, the inspection interval may be the full
remaining safe operating life up to a maximum of 2 years.

----------- Start Original Message -----------
: Hello,
: I am working on a Gas gathering platform offshore. We need to know the frequency of the pressel vessels inspection, internal visual...As per API510, what is the frequency of a vessel to be inspected which is 2 and half years old?Someone please advise.Is it once in 5 years?We have a shut down coming and planning has to be done.
------------ End Original Message ------------




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
05:31 Apr-11-2008
Re: API-510 Pressure vessels inspection frequency
There is no simple answer to this question and I recommend you study API closely. The first issue is whether there is any jursidictional rules that will override API 510. The law comes first. Then there are options within 510 as to whether you plan using Risk based Inspection or Time Based Maximum Intervals as shown in API 510.
The time based intervals in 510 state that you must do an inspection at time of installation and when the vessel changes service or ownership. An external inspection on an interval not exceeding 5 years. Internal inspections not exceeding half the remaining life or ten yeras. The internal may be replaced by an on-steam inspection if the criteria of Para 6.5.2.1 are met.

And of course an RBI program may increase or decrease these intervals depending upon the analysis.


 
 Reply 
 
Mr. Engineer
Mr. Engineer
01:50 Aug-28-2008
Re: API-510 Pressure vessels inspection frequency
In addition to API 510, if your vessel is in US waters note that US Code of Federal Regulations, 2007 “Shipping” 46 CFR Subpart 61.10-5 “Pressure vessels in service”
• basically for vessels with annual COI’s all pressure vessels listed on the COI shall be examined or tested every 5 years. This includes an external and internal examination however it does get specific on what is required by the external examination and I believe its up to the attending surveyor. If the vessel is equipped with a manhole or inspection port it must be opened and an internal examination also conducted. No hydrostatic test is required unless a defect is found that, in the marine inspectors opinion, may affect the safety of the pressure vessel.

Also note the class rules for which your vessel falls under but if its ABS then it will also require the same inspection on a 5 yr interval.


----------- Start Original Message -----------
: Hello,
: I am working on a Gas gathering platform offshore. We need to know the frequency of the pressel vessels inspection, internal visual...As per API 510, what is the frequency of a vessel to be inspected which is 2 and half years old?Someone please advise.Is it once in 5 years?We have a shut down coming and planning has to be done.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window