NDT methods for the structural foundation

I was searching information about present NDT methods for the inspection of civil engineering structural foundation.
i could not find any papers but one i have now. could anyone give me any references or information about this issue?

thank you very much


 
 Reply 
 
Edouard G. Nesvijski
R & D, Senior Scientist
TRS Technologies, USA, Joined Jan 2000, 9

Edouard G. Nesvijski

R & D, Senior Scientist
TRS Technologies,
USA,
Joined Jan 2000
9
04:47 Feb-15-2000
Re: NDT methods for the structural foundation
tive Evaluation: A Tool in Design, Manufacturing, and Service, CRC Press, 1997, -586 pages.

3. V. Dzenis. Application of the Ultrasonic Transducers with Point Contact for the Nondestructive Testing, "Zinatne" Publishing Houwe, Riga, Latvia, 1987, - 264 pages (in Russian).

Sincerely,
Edouard G. Nesvijski



 
 Reply 
 
Michael Dalichow
Michael Dalichow
06:33 Feb-16-2000
Re: NDT methods for the structural foundation
Dear Young:
The Fraunhofer-Institute Nondestructive Testing (IZFP) has developed a method to diagnose moisture content and distribution in concrete foundation using portable nondestructive teechniques. The "NMR-Inspect" system is based Hydrogen Nuclear Magnetic Resonance (1H-NMR).
Please contact Bernd Wolter at IZFP for more information by phone (+49 681 9302-3883) or email at wolter@izfp.fhg.de.



 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window