where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

TecScan Systems
We offer a complete line of NDT scanners, Immersion Tanks & Gantry systems which incorporate Ultrasonic, Phased Array & Eddy Current technologies.
2040 views
Technical Discussions
Doug Mendes
NDT Inspector, R & D
Imetrix Inc., USA, Joined Oct 1999, 7

Doug Mendes

NDT Inspector, R & D
Imetrix Inc.,
USA,
Joined Oct 1999
7
07:17 Feb-29-2000
Ultrasonic Modeling

I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

Thanks
Doug Mendes



 
 Reply 
 
John Rutter
John Rutter
01:36 Feb-29-2000
Re: Ultrasonic Modeling
I have not used this software, but it looks good. The folks at UTEX are quite helpful.

http://www.utex.com/pages/imagine3d/i3d.htm

-John Rutter



 
 Reply 
 
M. William Moyer
M. William Moyer
02:03 Feb-29-2000
Re: Ultrasonic Modeling
Wave2000 is another package that can do 2D modeling.
See the following URL for examples: http://www.cyberlogic.com


: I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: Thanks
: Doug Mendes




 
 Reply 
 
Jonathan J. Kaufman
Jonathan J. Kaufman
02:54 Feb-29-2000
Re: Ultrasonic Modeling
Imagine3D is a ray tracing program, and as such, does
not model all of the interactions associated with
ultrasonic propagation. It works pretty well in blocks
of homogeneous media (like layered media), but not so well
with flaws and model structures anywhere on the order
or several times the order of a wavelength. On the
other hand, Wave2000 models all the interactions
of ultrasound with a structure. This comes at a price,
however, the price of increased computational
overhead. But flaws and an ultrasound wavefront
interaction with it are computed without any signficant
error.

Please note: My company (Cyberlogic, Inc.) produces
and sells Wave2000.

Jonathan Kaufman


: I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: Thanks
: Doug Mendes




 
 Reply 
 
Hermann Landes
Hermann Landes
04:54 Mar-01-2000
Re: Ultrasonic Modeling
: I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: Thanks
: Doug Mendes

Dear Mr. Mendes,

a collegue from the university of Linz, Austria, forwarded me your inquiry on
ultrasonic modeling tools. We have developed the
finite-element-boundary-element simulation program CAPA, which is dedicated
to the modeling of electromechanical transducers (incl. piezoelectric,
magneto-mechanical and electrostatic), acoustic wave propagation in media at
rest and in flow (incl. nonlinear acoustic waves). This program is in use at
several industrial companies and universities, worldwide, allthough primarily
based in Europe. As far as I can see from your inquiry, these problems can be
simulated with our program very efficiently.
For a first information on CAPA, you may have a look at the web-page of the
institute of Prof. Lerch at the university of Erlangen. Just point your
browser to the following address:
http://www.lse.uni-erlangen.de/CAPA/index.htm.
We have also produced a CD providing an overview over the software system.
Furthermore, the slides of the shortcourse 'Computer modeling of
electromechanical transducers' held by Lerch, Kaltenbacher, and Landes at the
IEEE ultrasonics symposium in Lake Tahoe, October 1999, are also included. In
case that you are interested in this CD, please let me know. We would be
happy to send you a copy as well as some of our recent publications.

Yours sincerely

Hermann Landes
Wissenschaftliche Software
Eisenstr.35
D-91054 Buckenhof



 
 Reply 
 
ss
ss
09:57 Apr-28-2000
Re: Ultrasonic Modeling
: I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: Thanks
: Doug Mendes




 
 Reply 
 
Patricia Leggat
Patricia Leggat
00:29 Oct-09-2000
Re: Ultrasonic Modeling
I recently came across your posted question on the Forum. If you are still interested in software for ultrasonic modelling NDTSoft have software for 3D Ray Tracing in simple or complex solid model components. For more information please go to www.NDTSoft.co.uk or contact myself.

Patricia Leggat
PatriciaLeggat@NDTSoft.co.uk

: I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: Thanks
: Doug Mendes




 
 Reply 
 
Ehsan Sadigh Rad
Ehsan Sadigh Rad
06:01 Sep-16-2001
Re: Ultrasonic Modeling
: Imagine3D is a ray tracing program, and as such, does
: not model all of the interactions associated with
: ultrasonic propagation. It works pretty well in blocks
: of homogeneous media (like layered media), but not so well
: with flaws and model structures anywhere on the order
: or several times the order of a wavelength. On the
: other hand, Wave2000 models all the interactions
: of ultrasound with a structure. This comes at a price,
: however, the price of increased computational
: overhead. But flaws and an ultrasound wavefront
: interaction with it are computed without any signficant
: error.

: Please note: My company (Cyberlogic, Inc.) produces
: and sells Wave2000.

: Jonathan Kaufman

:
: : I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: : It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: : I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: : Thanks
: : Doug Mendes
: : I will be happy if I get a version of wave2000 saimulation program in any case.




 
 Reply 
 
Ehsan Sadigh Rad
Ehsan Sadigh Rad
06:03 Sep-16-2001
Re: Ultrasonic Modeling
: : I will be happy if I get a version of wave2000 saimulation program in any case.
Thanks , Ehsan S. Rad




 
 Reply 
 
Nihat Kurkcu
Engineering
Turkey, Joined Jul 2001, 4

Nihat Kurkcu

Engineering
Turkey,
Joined Jul 2001
4
08:39 Sep-17-2001
Re: Ultrasonic Modeling
I am also interested in modeling Ultrasonics.
I would like to have more information about your wave2000 software. If possible, i would like to know the mathematical base of the model,too. The problem is how accurate is the model? There are still problems in solving the equations.
Do you have any webpage describing your software?
If it is a problem talking about the mathematical base;
Basically:
1- Does your model cover immersion ultrasonic inspections
2- Is it possible to run the model both for isotropic and anisotropic materials
3- Have you done any validation including different defects?
4- Does it caover composite materials?
Thank you very much
Nihat
NDE Engineer
GEAE/GE MRC


Imagine3D is a ray tracing program, and as such, does
: not model all of the interactions associated with
: ultrasonic propagation. It works pretty well in blocks
: of homogeneous media (like layered media), but not so well
: with flaws and model structures anywhere on the order
: or several times the order of a wavelength. On the
: other hand, Wave2000 models all the interactions
: of ultrasound with a structure. This comes at a price,
: however, the price of increased computational
: overhead. But flaws and an ultrasound wavefront
: interaction with it are computed without any signficant
: error.

: Please note: My company (Cyberlogic, Inc.) produces
: and sells Wave2000.

: Jonathan Kaufman

:
: : I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.

: : It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.

: : I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?

: : Thanks
: : Doug Mendes




 
 Reply 
 
Jonathan J. Kaufman
Jonathan J. Kaufman
06:08 Jan-05-2002
Re: Ultrasonic Modeling
We produce Wave2000, a 2D ultrasound simulation
package. We are also developing Wave2500, a 3D-
axisymmetric package, which will be ready soon.

A demo is available on our web site
(www.cyberlogic.org)

In answer to your questions:

right now the software handles only isotropic
materials.

composite materials can be modelled, but then you
would need to model each component separately (eg,
layer by layer).

fluids and solids are modelled, so immersion type
measurements are not a problem.

the program has been shown to produce results
consistent with a wide range of experiments.

please feel free to contact us if you would like
any additional info.


: I am also interested in modeling Ultrasonics.
: I would like to have more information about your wave2000 software. If possible, i would like to know the mathematical base of the model,too. The problem is how accurate is the model? There are still problems in solving the equations.
: Do you have any webpage describing your software?
: If it is a problem talking about the mathematical base;
: Basically:
: 1- Does your model cover immersion ultrasonic inspections
: 2- Is it possible to run the model both for isotropic and anisotropic materials
: 3- Have you done any validation including different defects?
: 4- Does it caover composite materials?
: Thank you very much
: Nihat
: NDE Engineer
: GEAE/GE MRC
.
:
: Imagine3D is a ray tracing program, and as such, does
: : not model all of the interactions associated with
: : ultrasonic propagation. It works pretty well in blocks
: : of homogeneous media (like layered media), but not so well
: : with flaws and model structures anywhere on the order
: : or several times the order of a wavelength. On the
: : other hand, Wave2000 models all the interactions
: : of ultrasound with a structure. This comes at a price,
: : however, the price of increased computational
: : overhead. But flaws and an ultrasound wavefront
: : interaction with it are computed without any signficant
: : error.
.
: : Please note: My company (Cyberlogic, Inc.) produces
: : and sells Wave2000.
.
: : Jonathan Kaufman
.
: :
: : : I'm interested in information on ultrasonic modeling (simulation) programs for use in technique development and signal interpretation of structures with complex geometries that are accesible from only one side.
.
: : : It seems that there is increasing mention of models and simulations circulating throughout various discussion groups and its quite obvious to me the benefits of these programs to certain applications.
.
: : : I'm curious as to how reliable and useful these programs could be and whether there are currently any available for purchase for indivudual use?
.
: : : Thanks
: : : Doug Mendes
.



 
 Reply 
 
Govind Sharma
Govind Sharma
03:03 Nov-06-2002
Re: Ultrasonic Modeling
: I am also interested in modeling Ultrasonics.
: I would like to have more information about your wave2000 software. If possible, i would like to know the mathematical base of the model,too. The problem is how accurate is the model? There are still problems in solving the equations.

: Do you have any webpage describing your software?
: If it is a problem talking about the mathematical base;
: Basically:
: 1- can i use this in weld joits study also?
: 2- Does your model cover immersion ultrasonic inspections
: 3- Is it possible to run the model both for isotropic and anisotropic materials
: 4- Have you done any validation including different defects?
: 5- Does it caover composite materials?
: 6 - can i view the wave inside the material?
: Thank you very much
: Govind Sharma
: Scientific officer
NDT&E Division
Kalpakkam
.
:
:


 
 Reply 
 

Product Spotlight

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

New PHAsis module for longitudinal weld seam inspection

PHAsis® Phased Array manual ultrasonic spot weld inspection device is now ideally suited for test
...
ing of longitudinally welded seams (e.g. Arplas® seam, short line seams) with a length of 3 to 12 mm.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window