mj
mj
08:58 Jun-08-2008
CHIME

all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated


 
 Reply 
 
bob sudharmn
Engineering, Reliability and Integrity Eng
Shell Malaysia Trading, Malaysia, Joined Jan 2008, 54

bob sudharmn

Engineering, Reliability and Integrity Eng
Shell Malaysia Trading,
Malaysia,
Joined Jan 2008
54
01:55 Jun-09-2008
Re: CHIME
There is an article on this subject. Refer attached link

http://www.ndt.net/article/ecndt98/chemical/103/103.htm


----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 283

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
283
03:53 Jun-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.

As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.



 
 Reply 
 
mj
mj
08:43 Jun-10-2008
Re: CHIME
Dear Mr. John,
Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?


----------- Start Original Message -----------
: : all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
: CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.
: As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.
------------ End Original Message ------------




 
 Reply 
 
Mark Nel
Mark Nel
03:14 Jun-10-2008
Re: CHIME
Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
----------- Start Original Message -----------
: Dear Mr. John,
: Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?



 
 Reply 
 
Charlie Lawther
Charlie Lawther
02:24 Jun-12-2008
Re: CHIME
CHIME is manufactured by ESR (Was AEA Technology) They could provide you with equipment and a license to use CHIME.

3 companies currently have a license to use this equipment.
----------- Start Original Message -----------
: Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
: : Dear Mr. John,
: : Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?
------------ End Original Message ------------




 
 Reply 
 
RT. Jeyakumar
RT. Jeyakumar
07:59 Jul-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

Good day MJ,

Olympus (RD Tech, Canada) is manufacturing equipment with CHIME software. It is user friendly too. It is no other than Olympus multi scan equipment with TOFD, CHIME, Eddy Current (Surface scanning), etc. Hope you're MJ of Malaysia. If so, contact Olympus Singapore. They can help you

Regards,

RT. Jeyakumar


 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window