mj
mj
08:58 Jun-08-2008
CHIME

all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated


 
 Reply 
 
bob sudharmn
Engineering, Reliability and Integrity Eng
Shell Malaysia Trading, Malaysia, Joined Jan 2008, 54

bob sudharmn

Engineering, Reliability and Integrity Eng
Shell Malaysia Trading,
Malaysia,
Joined Jan 2008
54
01:55 Jun-09-2008
Re: CHIME
There is an article on this subject. Refer attached link

http://www.ndt.net/article/ecndt98/chemical/103/103.htm


----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 281

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
281
03:53 Jun-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.

As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.



 
 Reply 
 
mj
mj
08:43 Jun-10-2008
Re: CHIME
Dear Mr. John,
Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?


----------- Start Original Message -----------
: : all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
: CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.
: As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.
------------ End Original Message ------------




 
 Reply 
 
Mark Nel
Mark Nel
03:14 Jun-10-2008
Re: CHIME
Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
----------- Start Original Message -----------
: Dear Mr. John,
: Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?



 
 Reply 
 
Charlie Lawther
Charlie Lawther
02:24 Jun-12-2008
Re: CHIME
CHIME is manufactured by ESR (Was AEA Technology) They could provide you with equipment and a license to use CHIME.

3 companies currently have a license to use this equipment.
----------- Start Original Message -----------
: Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
: : Dear Mr. John,
: : Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?
------------ End Original Message ------------




 
 Reply 
 
RT. Jeyakumar
RT. Jeyakumar
07:59 Jul-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

Good day MJ,

Olympus (RD Tech, Canada) is manufacturing equipment with CHIME software. It is user friendly too. It is no other than Olympus multi scan equipment with TOFD, CHIME, Eddy Current (Surface scanning), etc. Hope you're MJ of Malaysia. If so, contact Olympus Singapore. They can help you

Regards,

RT. Jeyakumar


 
 Reply 
 

Product Spotlight

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window