Technical Discussions
mj
mj
08:58 Jun-08-2008
CHIME

all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated


 
 Reply 
 
bob sudharmn
Engineering, Reliability and Integrity Eng
Shell Malaysia Trading, Malaysia, Joined Jan 2008, 54

bob sudharmn

Engineering, Reliability and Integrity Eng
Shell Malaysia Trading,
Malaysia,
Joined Jan 2008
54
01:55 Jun-09-2008
Re: CHIME
There is an article on this subject. Refer attached link

http://www.ndt.net/article/ecndt98/chemical/103/103.htm


----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 281

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
281
03:53 Jun-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.

As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.



 
 Reply 
 
mj
mj
08:43 Jun-10-2008
Re: CHIME
Dear Mr. John,
Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?


----------- Start Original Message -----------
: : all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
: CHIME is not so much an equipment but a technique based on the correct transducers, wave modes, data display and interpretation. The technique was developed by the HOIS JIP when it was part of AEA Technology. HOIS 2000 is now part of ESR Technology based in Abingdon Oxfordshire.
: As indicated in an earlier posting there are published papers on the technique and some of the computer based UT system manufacturers now offer CHIME capabilities.
------------ End Original Message ------------




 
 Reply 
 
Mark Nel
Mark Nel
03:14 Jun-10-2008
Re: CHIME
Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
----------- Start Original Message -----------
: Dear Mr. John,
: Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?



 
 Reply 
 
Charlie Lawther
Charlie Lawther
02:24 Jun-12-2008
Re: CHIME
CHIME is manufactured by ESR (Was AEA Technology) They could provide you with equipment and a license to use CHIME.

3 companies currently have a license to use this equipment.
----------- Start Original Message -----------
: Try AGR Field Operations, we supply equipment and software for the CHIME technique. Our Aberdeen and Bergen offices also provide site service using CHIME amongst other NDT services. The data needs to be processed & presented in a computer generated format that would not be possible on conventional flaw detectors.
: : Dear Mr. John,
: : Can you please help me to find out the manufacture for CHIME equipment? is it possible to do chime with Normal Ultrasonic equipment?
------------ End Original Message ------------




 
 Reply 
 
RT. Jeyakumar
RT. Jeyakumar
07:59 Jul-09-2008
Re: CHIME
----------- Start Original Message -----------
: all my specialist friends... can i get some information of CHIME Rapid screening system. and who's the manufacture, any news about this equipment is highly appricated
------------ End Original Message ------------

Good day MJ,

Olympus (RD Tech, Canada) is manufacturing equipment with CHIME software. It is user friendly too. It is no other than Olympus multi scan equipment with TOFD, CHIME, Eddy Current (Surface scanning), etc. Hope you're MJ of Malaysia. If so, contact Olympus Singapore. They can help you

Regards,

RT. Jeyakumar


 
 Reply 
 

Product Spotlight

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...