Flexible risers

I am new to this forum, but have interest in a subject last time disussed in Nov.98 - inspection tools and references for flexible risers. This is an increasing need for the offshore oil&gas market - and my company are involved in developing equipment for this purpose. Any reply will be of interest

stein erik kvam


 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1286

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1286
04:15 Mar-07-2000
Re: Flexible risers
Erik:
Could you please provide more details on the needs of your particular application.
It is my understanding that offshore catenary risers are subject to cyclic fatique stresses and tensile stresses.
This makes surface breaking flaws very critical.
Welded joints on risers are presently being tested using mechanised UT using zonal discrimination.
Is this applicable to your situation?

Ed

: I am new to this forum, but have interest in a subject last time disussed in Nov.98 - inspection tools and references for flexible risers. This is an increasing need for the offshore oil&gas market - and my company are involved in developing equipment for this purpose. Any reply will be of interest

: stein erik kvam




 
 Reply 
 

Product Spotlight

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

High-end Ultrasonic Flaw Detector with 32:128PR PAUT and 2-ch TOFD: SyncScan 2

SIUI’s newly launched SyncScan 2, is a high-end ultrasonic flaw detector with 32:128PR PAUT and
...
2-ch TOFD, which can maximize your efficiency for PA and TOFD. ● Support PA/TOFD/UT ● 32-ch PA is more suitable for inspection on extra-thick wall and high-attenuation material. ● 32-ch PA and 2-ch TOFD work simultaneously. ● Support PR mode for corrosion inspection.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window