Technical Discussions
M.C Macke
NDT Inspector
GE Inspection Services, USA, Joined Aug 2001, 8

M.C Macke

NDT Inspector
GE Inspection Services,
USA,
Joined Aug 2001
8
06:57 Mar-13-2000
Hi Temp thickness of enamle on carbon.

Without touching the piece, it is of major interest to know the
thickness of the enamle coating on cast iron. The maximum thickness
is 3mm. The key is to know this thickness at the initial
solidification temp of 1000f...if there is to little, then he can
add (t), this will help reduce the heating cycles and improve
the Quality control. This system can be assemply line driven if
proven reliable. The problems are 1000f and no contact. Emat is
out, contact required! Mag Lift off...no! UT..2 TO 3 mm at 1000f,
I don't know? Could Infrared be of some help or other optical
method? This one is giving me a hard time of it!!!!




 
 Reply 
 
M. William Moyer
M. William Moyer
07:04 Mar-13-2000
Re: Hi Temp thickness of enamle on carbon.
I saw something recently where laser ultrasonics was used to measure
wet paint thickness. Perhaps it would also work here.


: Without touching the piece, it is of major interest to know the
: thickness of the enamle coating on cast iron. The maximum thickness
: is 3mm. The key is to know this thickness at the initial
: solidification temp of 1000f...if there is to little, then he can
: add (t), this will help reduce the heating cycles and improve
: the Quality control. This system can be assemply line driven if
: proven reliable. The problems are 1000f and no contact. Emat is
: out, contact required! Mag Lift off...no! UT..2 TO 3 mm at 1000f,
: I don't know? Could Infrared be of some help or other optical
: method? This one is giving me a hard time of it!!!!




 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 609

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
609
06:47 Mar-14-2000
Re: Hi Temp thickness of enamle on carbon.
: Without touching the piece, it is of major interest to know the
: thickness of the enamle coating on cast iron. The maximum thickness
: is 3mm. The key is to know this thickness at the initial
: solidification temp of 1000f...if there is to little, then he can
: add (t), this will help reduce the heating cycles and improve
: the Quality control. This system can be assemply line driven if
: proven reliable. The problems are 1000f and no contact. Emat is
: out, contact required! Mag Lift off...no! UT..2 TO 3 mm at 1000f,
: I don't know? Could Infrared be of some help or other optical
: method? This one is giving me a hard time of it!!!!
----------------

Be carefully by measuring under such hot conditions.
You can get calibration errors of sound velocity, also
the circumferential temperature may not be equal.
There is a company 'MOOG-BUHL AUTOMATION' which supplied
ultrasonic in this field, but measured more down the line.

Rolf



 
 Reply 
 

Product Spotlight

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window