Technical Discussions
gowrishankar
R & D, scientist
ISRO, India, Joined Nov 2008, 34

gowrishankar

R & D, scientist
ISRO,
India,
Joined Nov 2008
34
02:32 Aug-08-2008
x ray

sir,
i would like to know upto which thickness in steel we can take radiodraphs with 2 percentage sensitivity?
what is its limitation?
In other way we have a 0.5mm thin welding (by just fusion without filler wire) Can we assess this weld quality by Xray radiography?
pl give me details?



 
 Reply 
 
Nigel
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
07:03 Aug-08-2008
Re: x ray
From your second question it seems you have access to X-ray equipment. With X-ray and some exposure parameter tweaking you should always be able to achieve 2% sensitivity. The only limitation will be the maximum steel thickness your X-ray equipment will penetrate. For your 0.5mm thick (steel?) weld, low kV X-ray can give you excellent results. If you wish to penetrate much thicker steel sections then, assuming you only have access to isotopes, you will need to make test shots to detemine the capability of the set-up to achieve 2% sensitivity. Factors affecting sensitivity are film and subject contrast and definition, so you need to consider all the factors which control those parameters, such as kV, filtering, scatter control, film speed. Dont you have exposure charts for the equipment and film you are working with?

Try a few test shots with the equipment materials you have to hand - seeing is believing and altering parameters and seeing the results will give you a good idea what you will need to do for production.

Regards

Nigel

----------- Start Original Message -----------
: sir,
: i would like to know upto which thickness in steel we can take radiodraphs with 2 percentage sensitivity?
: what is its limitation?
: In other way we have a 0.5mm thin welding (by just fusion without filler wire) Can we assess this weld quality by Xray radiography?
: pl give me details?
------------ End Original Message ------------




 
 Reply 
 
Afshun Agha Amiri
Afshun Agha Amiri
01:38 Aug-09-2008
Re: x ray
----------- Start Original Message -----------
Dear Friend,
In industrial RT For proper recommendations about energy selection and relevant thickness limitation on steel materials,you can refer to some code/standards(such as BS/EN1435 or old version of ASMEsec.5-before 1998),ASNT RT handbook,ASM handbook(vol.17)and others reference books.
2%sensitivity means : as a RT quality criteria and be checked by IQI,is 2% of test material thickness which is minimum detectable defect size through thickness.
you may obtain 2% sensitivity by x-ray or gamma-ray.
You can refer to ASM handbook(vol.17).


 
 Reply 
 
gowrishankar
R & D, scientist
ISRO, India, Joined Nov 2008, 34

gowrishankar

R & D, scientist
ISRO,
India,
Joined Nov 2008
34
06:31 Aug-12-2008
Re: x ray
Thank you sirs,
regards
gowrishankar

----------- Start Original Message -----------
: Dear Friend,
: In industrial RT For proper recommendations about energy selection and relevant thickness limitation on steel materials,you can refer to some code/standards(such as BS/EN1435 or old version of ASMEsec.5-before 1998),ASNT RT handbook,ASM handbook(vol.17)and others reference books.
: 2%sensitivity means : as a RT quality criteria and be checked by IQI,is 2% of test material thickness which is minimum detectable defect size through thickness.
: you may obtain 2% sensitivity by x-ray or gamma-ray.
: You can refer to ASM handbook(vol.17).
------------ End Original Message ------------




 
 Reply 
 
tj
tj
03:20 Nov-14-2008
Re: x ray
----------- Start Original Message -----------
: Dear Friend,
: In industrial RT For proper recommendations about energy selection and relevant thickness limitation on steel materials,you can refer to some code/standards(such as BS/EN1435 or old version of ASMEsec.5-before 1998),ASNT RT handbook,ASM handbook(vol.17)and others reference books.
: 2%sensitivity means : as a RT quality criteria and be checked by IQI,is 2% of test material thickness which is minimum detectable defect size through thickness.
: you may obtain 2% sensitivity by x-ray or gamma-ray.
: You can refer to ASM handbook(vol.17).
------------ End Original Message ------------

This could be misleading. You should never rely on your IQI as a gauge of minimum defect size. Your acceptance criteria and the quality indicator are two seperate issues.


 
 Reply 
 

Product Spotlight

Customized Probes and Transducers

With a strong development department and our own piezocomposite production, we accompany you from th
...
e first product idea to serial production. Our scientists are continuously researching new methods in the field of ultrasonic measurement technology. The progress achieved enables us to offer you optimal solutions.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window