Aluminum Casting NDT Suggestions

I am a student in the United States and new to non-destructive testing techniques. Can you suggest available (or easily modifiable) methods to test C355 aluminum cast parts - specifically turbocharger compressor wheels. The method should be relatively inexpensive, reliable, and easily interpretable.

Thanks
Sandy Coldwell
(a starving Mechanical Engineering student)
ws.coldwell@prodigy.net


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
09:34 Sep-28-1999
Re: Aluminum Casting NDT Suggestions

: I am a student in the United States and new to non-destructive testing techniques. Can you suggest available (or easily modifiable) methods to test C355 aluminum cast parts - specifically turbocharger compressor wheels. The method should be relatively inexpensive, reliable, and easily interpretable.

Are you looking to perform thickness gaging, flaw detection, or material properties analysis? It is possible that common ultrasonic NDT techniques using off-the-shelf equipment could be employed for all three, but I'd need more information on exactly what you're trying to do to say more. If it's thickness gaging, we would need to know the thickness range, resolution/accuracy requirements, and whether there were any geometrical limitations like non-parallel walls or restricted access for probes. For flaw detection, we'd need to know the EXACT part geometry as well as the type, location, minimum size, and geometry of the anomalies that you're looking for. For material properties, ultrasonic techniques can often be used to quantify elastic modulus, as well as for analyzing grain size and distribution and a few other less common tests.

Based on a further definition of your test requirements, possibly followed by evaluation of representative samples of the parts in question, ultrasonic equipment from companies like mine may meet your needs.

--Tom Nelligan



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 304

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
304
08:09 Sep-29-1999
Re: Aluminum Casting NDT Suggestions
: I am a student in the United States and new to non-destructive testing techniques. Can you suggest available (or easily modifiable) methods to test C355 aluminum cast parts - specifically turbocharger compressor wheels. The method should be relatively inexpensive, reliable, and easily interpretable.

: Thanks
: Sandy Coldwell
: (a starving Mechanical Engineering student)

Our company is using Resonant Inspection in inspecting many different component types for customers.
This is mainly used in testing mass produced components, especially for the automotive industry.

I have looked at cast Turbocharger Compressors for another customer, and have concluded that we could probably test these parts also, but the tests would probably have to be carried out before the balancing process of manufacturing.
We expect to detect cracks and also internal porosity, provided that the defects are sufficiently serious enough to have ANY effect on the structural integrity of the part.
If the defects do not have an effect on this, then we do not detect them (and you probably dont want to reject these parts).

The test would (after setting it up) provide a Go-NoGo signal for acceptance and rejection. Testing times typically of 3 to 6 seconds per piece are normal, and when looking at mass produced parts, payback of the systems are usually realised within 12 to 18 months, sometimes less.

Let me have some details, and I will get our USA contact to get in touch.

Regards,

Godfrey Hands





 
 Reply 
 
Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
00:33 Dec-02-1999
Re: Aluminum Casting NDT Suggestions
One method is digital radiography. I am with the University of Alabama in Birmingham. We are performing UT and Radiography on casting and then eveluating digital radiography for feature characterization.

You may call me at (205) 714-3701.

Sincerely,

J. Mark Davis




 
 Reply 
 
Eng. Fathi Ghanameh
Eng. Fathi Ghanameh
02:25 Dec-23-1999
Re: Aluminum Casting NDT Suggestions
: I am a student in the United States and new to non-destructive testing techniques. Can you suggest available (or easily modifiable) methods to test C355 aluminum cast parts - specifically turbocharger compressor wheels. The method should be relatively inexpensive, reliable, and easily interpretable.

: Thanks
: Sandy Coldwell
: (a starving Mechanical Engineering student)
: ws.coldwell@prodigy.net




 
 Reply 
 
jason scott
jason scott
00:11 Mar-27-2000
Re: Aluminum Casting NDT Suggestions
penetrant tests will give you quite accurate results for surface breaking flaws, this can be very portable or usuually involves the use of fluorescent inspection within the aerospace industry, this method isn't as portable but very effective

radiography is also used on this kind of part and also effective especially for volumetric type flaws, this would generally be quite expensive though depending on local resources

if i can be of any furthe assistance contact me on the above e-mail address


 
 Reply 
 
behrooz movahedi
behrooz movahedi
08:27 Mar-02-2002
Re: Aluminum Casting NDT Suggestions
: I am a student in the isfahan university of technology and new to non-destructive testing techniques. Can you suggest available (or easily modifiable) methods to test C355 aluminum cast parts - specifically turbocharger compressor wheels. The method should be relatively inexpensive, reliable, and easily interpretable.

: Thanks
: behrooz movahedi
: DEBT.MATERIALS ENG.



 
 Reply 
 

Product Spotlight

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

AMIGO2

TSC Amigo2 - ACFM technology has developed a solid reputation for accurately detecting and sizing
...
surface-breaking cracks through paint and coatings. As the industry demands increased performance in speed, signal quality, and portability, it’s time for an evolution. It’s time for Amigo2.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window