Shibu T James
Shibu T James
02:56 Sep-10-2008
100% RT on process piping

Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
05:53 Sep-10-2008
Re: 100% RT on process piping
Hi Shibu

Code B31.3. requires 100% RT under severe cyclic conditions and for Chapter IX, High Pressure Piping.

Your 2nd sentence should bear a warning as it falls short of the total requirements for closure (golden) welds, para 345.9, and also the conditions under which hydrotest may be omitted, para. 345.1(c). There is also a requirement for flexibility analysis and senstitive leak test plus any further Owner-imposed requirements such as in-process examination.

You ask when "we can request" 100% RT. Do you mean the Owner as defined by ASME? If its not a specific Code requirement as in the case of normal fluid service (5% random RT), but the Owner wants the extra confidence through 100% RT then this should be stipulated at the FEED stage so that there will be no "Its non-contractual so either we wont do it or we shall re-charge" from your inspection contractor.

Hope this helps

Nigel


----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping inlieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------




 
 Reply 
 
Rafal Mis
Sales, - Technical Support
Olympus Poland, Poland, Joined Sep 2008, 12

Rafal Mis

Sales, - Technical Support
Olympus Poland,
Poland,
Joined Sep 2008
12
08:25 Sep-11-2008
Re: 100% RT on process piping
----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------

I'd like to put in the picture UT of pipes instead of RT. Some companies accept special IBUS-TD method for UT of thin pipe welds. This method in very sensitive, reliable and is much cheaper than RT. If this post gave you any help than please write to me for additional informations.


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
03:45 Sep-11-2008
Re: 100% RT on process piping
----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------

The ASME Codes are a minimum set of standard requirements and should always be part of a wider engineering set of specifications developed by the owner to fully cover the intended application. The owner can always increase the required degree or type of examination above the minimum code requirements its just a question of are you willing to pay for it. Remember its often not just the cost of examination that contractors may want to recover they may want to increase their allowance for re-work especially on lump sum jobs to allow for the fact that the increased examination may find more items requiring repair.


 
 Reply 
 
Ed T.
Ed T.
03:12 Sep-12-2008
Re: 100% RT on process piping
I have been pon projects where the final welds or "Golden Welds" get 100% RT in lieu of hydrotesting. I have also seen situations where we were tying into an existing line. The owner was concerned the existing line was old and may not take the hydrotest pressure so we would perform 100% RT in lieu of hydro.
This is awlway agreed to before the work is perfomed though.

----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------




 
 Reply 
 
fadhilhasb
fadhilhasb
07:33 Jul-07-2017
Re: 100% RT on process piping
In Reply to Shibu T James at 02:56 Sep-10-2008 (Opening).

In ASME B31.4 or B31.8. That have statement show when perform 100% RT for piping can waive Hydrotest requirement?

 
 Reply 
 
Steven Doc
Other, Quality Manager
Siemens Energy, Egypt, Joined Feb 2011, 187

Steven Doc

Other, Quality Manager
Siemens Energy,
Egypt,
Joined Feb 2011
187
17:49 Jul-10-2017
Re: 100% RT on process piping
In Reply to fadhilhasb at 07:33 Jul-07-2017 .

Personally I would not accept RT in lieu of Hydrotest. They are completely different examinations resulting in completely different outputs.

100% RT only tells us if the welder has performed to pre determined workmanship standards, it tells zero about the integrity of the weld.

 
 Reply 
 

Product Spotlight

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window