100% RT on process piping

Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?


 
 Reply 
 
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
05:53 Sep-10-2008
Re: 100% RT on process piping
Hi Shibu

Code B31.3. requires 100% RT under severe cyclic conditions and for Chapter IX, High Pressure Piping.

Your 2nd sentence should bear a warning as it falls short of the total requirements for closure (golden) welds, para 345.9, and also the conditions under which hydrotest may be omitted, para. 345.1(c). There is also a requirement for flexibility analysis and senstitive leak test plus any further Owner-imposed requirements such as in-process examination.

You ask when "we can request" 100% RT. Do you mean the Owner as defined by ASME? If its not a specific Code requirement as in the case of normal fluid service (5% random RT), but the Owner wants the extra confidence through 100% RT then this should be stipulated at the FEED stage so that there will be no "Its non-contractual so either we wont do it or we shall re-charge" from your inspection contractor.

Hope this helps

Nigel


----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping inlieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------




 
 Reply 
 
Rafal Mis
Sales, - Technical Support
Olympus Poland, Poland, Joined Sep 2008, 12

Rafal Mis

Sales, - Technical Support
Olympus Poland,
Poland,
Joined Sep 2008
12
08:25 Sep-11-2008
Re: 100% RT on process piping
----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------

I'd like to put in the picture UT of pipes instead of RT. Some companies accept special IBUS-TD method for UT of thin pipe welds. This method in very sensitive, reliable and is much cheaper than RT. If this post gave you any help than please write to me for additional informations.


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
03:45 Sep-11-2008
Re: 100% RT on process piping
----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------

The ASME Codes are a minimum set of standard requirements and should always be part of a wider engineering set of specifications developed by the owner to fully cover the intended application. The owner can always increase the required degree or type of examination above the minimum code requirements its just a question of are you willing to pay for it. Remember its often not just the cost of examination that contractors may want to recover they may want to increase their allowance for re-work especially on lump sum jobs to allow for the fact that the increased examination may find more items requiring repair.


 
 Reply 
 
Ed T.
Ed T.
03:12 Sep-12-2008
Re: 100% RT on process piping
I have been pon projects where the final welds or "Golden Welds" get 100% RT in lieu of hydrotesting. I have also seen situations where we were tying into an existing line. The owner was concerned the existing line was old and may not take the hydrotest pressure so we would perform 100% RT in lieu of hydro.
This is awlway agreed to before the work is perfomed though.

----------- Start Original Message -----------
: Can you help me? 100% RT required for process piping in lieu of hydro test, do you know any other circumstances we can request for 100% RT for butt weld joints?
------------ End Original Message ------------




 
 Reply 
 
fadhilhasb
fadhilhasb
07:33 Jul-07-2017
Re: 100% RT on process piping
In Reply to Shibu T James at 02:56 Sep-10-2008 (Opening).

In ASME B31.4 or B31.8. That have statement show when perform 100% RT for piping can waive Hydrotest requirement?

 
 Reply 
 
Steven Doc
Other, Quality Manager
Siemens Energy, Egypt, Joined Feb 2011, 187

Steven Doc

Other, Quality Manager
Siemens Energy,
Egypt,
Joined Feb 2011
187
17:49 Jul-10-2017
Re: 100% RT on process piping
In Reply to fadhilhasb at 07:33 Jul-07-2017 .

Personally I would not accept RT in lieu of Hydrotest. They are completely different examinations resulting in completely different outputs.

100% RT only tells us if the welder has performed to pre determined workmanship standards, it tells zero about the integrity of the weld.

 
 Reply 
 

Product Spotlight

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window