Measuring Coating Thickness at Hig Temps

Im currently looking for an instrument to read thickness of a non-ferrous coating on a ferrous substrate, with a surface temp of 500 F. Magnetic gauges only go to 400F and are affected by high temp. Can anyone suggest a product?


 
 Reply 
 
Joseph P
Joseph P
03:58 Apr-27-2000
Re: Measuring Coating Thickness at Hig Temps
: Im currently looking for an instrument to read thickness of a non-ferrous coating on a ferrous substrate, with a surface temp of 500 F. Magnetic gauges only go to 400F and are affected by high temp. Can anyone suggest a product?




 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
04:00 Apr-27-2000
Measuring Coating Thickness at High Temps
The Lixi Profiler can measure at high temperature the thickness of a coating on ferrous material if the X-Ray absorption of the coating is at least 2% of the ferrous material


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
05:04 Apr-27-2000
Re: Measuring Coating Thickness at Hig Temps
: Im currently looking for an instrument to read thickness of a non-ferrous coating on a ferrous substrate, with a surface temp of 500 F. Magnetic gauges only go to 400F and are affected by high temp. Can anyone suggest a product?

What is the coating material and what is the thickness range? It may be possible to do this ultrasonically, using a high temperature delay line transducer, but I need more information about exactly what you're measuring to comment further.

--Tom Nelligan
Panametrics, Inc.




 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Content on Demand by Eddyfi Technologies

Finding yourself in front of a screen practicing safe social distancing instead of out in the fiel
...
d? At Eddyfi Technologies, we are doing our part in helping you be better prepared for what comes next. We introduce to you Eddyfi on Demand. Fill your schedule with webinars, how-to videos, informative technical papers and our NEW addition: Eddyfi Academy. There, you will have access to FREE online courses and obtain certificates of attendance once completed in order for you to include these e-learning sessions in your log of required training hours. Join us today. Stay safe, stay Beyond Current.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window