where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
1033 views
Technical Discussions
Mahesh Patel
Mahesh Patel
01:32 Apr-27-2000
Measuring Coating Thickness at Hig Temps

Im currently looking for an instrument to read thickness of a non-ferrous coating on a ferrous substrate, with a surface temp of 500 F. Magnetic gauges only go to 400F and are affected by high temp. Can anyone suggest a product?


 
 Reply 
 
Joseph P
Joseph P
03:58 Apr-27-2000
Re: Measuring Coating Thickness at Hig Temps
: Im currently looking for an instrument to read thickness of a non-ferrous coating on a ferrous substrate, with a surface temp of 500 F. Magnetic gauges only go to 400F and are affected by high temp. Can anyone suggest a product?




 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
04:00 Apr-27-2000
Measuring Coating Thickness at High Temps
The Lixi Profiler can measure at high temperature the thickness of a coating on ferrous material if the X-Ray absorption of the coating is at least 2% of the ferrous material


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
05:04 Apr-27-2000
Re: Measuring Coating Thickness at Hig Temps
: Im currently looking for an instrument to read thickness of a non-ferrous coating on a ferrous substrate, with a surface temp of 500 F. Magnetic gauges only go to 400F and are affected by high temp. Can anyone suggest a product?

What is the coating material and what is the thickness range? It may be possible to do this ultrasonically, using a high temperature delay line transducer, but I need more information about exactly what you're measuring to comment further.

--Tom Nelligan
Panametrics, Inc.




 
 Reply 
 

Product Spotlight

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window