Maximum penetration of Ir-192 in steel

Hi,
We are using Ir-192 to examine the casting quality of a steel part with maximum thickness 95.25mm:
(1) Is Ir-192 OK for this application?
(2) Does the decay influence the maximum penetration thickness?
Many thanks,
Pengzhu



 
 Reply 
 
tj
tj
07:11 Nov-14-2008
Re: Maximum penetration of Ir-192 in steel
----------- Start Original Message -----------
: Hi,
: We are using Ir-192 to examine the casting quality of a steel part with maximum thickness 95.25mm:
: (1) Is Ir-192 OK for this application?
: (2) Does the decay influence the maximum penetration thickness?
: Many thanks,
: Pengzhu
------------ End Original Message ------------

This would be working at the upper practical limit of Ir192. The energy levels would remain the same with decay. However, with loss of activity comes increased shot time and at 3in. of steel it would be impractical for normal use. Better to use higher energy x-ray or cobalt60 gamma.


 
 Reply 
 
Juan Amado
Engineering, Inspection
Arco Industrial, S.A., Panama, Joined Nov 2001, 44

Juan Amado

Engineering, Inspection
Arco Industrial, S.A.,
Panama,
Joined Nov 2001
44
09:53 Nov-14-2008
Re: Maximum penetration of Ir-192 in steel
----------- Start Original Message -----------
: : Hi,
: : We are using Ir-192 to examine the casting quality of a steel part with maximum thickness 95.25mm:
: : (1) Is Ir-192 OK for this application?
: : (2) Does the decay influence the maximum penetration thickness?
: : Many thanks,
: : Pengzhu
: This would be working at the upper practical limit of Ir192. The energy levels would remain the same with decay. However, with loss of activity comes increased shot time and at 3in. of steel it would be impractical for normal use. Better to use higher energy x-ray or cobalt60 gamma.
------------ End Original Message ------------


If 95mm is the maximum thickness, but you have thinner sections, you could probably gain valuable information about the part using Ir192, however, if you are looking to get a good density reading at the thickest portion of the casting you probably will not get it with this source.
Hope this helps, regards,
Juan Amado



 
 Reply 
 
Peter Alfers
Peter Alfers
09:53 Nov-16-2008
Re: Maximum penetration of Ir-192 in steel
you can use Ir 192 in conjunction with two Films how will
exposure at once. Than you need the half time for your right density .For the interpretation use the films lying upon each other.


 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window