Johan Blomkvist
Johan Blomkvist
09:25 Jun-15-2000
Inspection of lamppost`s

I would like to inspect lamppost´s for corrosion under ground level on the outside.
Which metod should i prefer?


 
 Reply 
 
Joseph Pascente
Joseph Pascente
05:36 Jun-15-2000
Re: Inspection of lamppost`s

Lixi Profiler can make this measurement for wall
thickness on ourdoor lamp posts.


Regards,

Joe Pascente

: I would like to inspect lamppost´s for corrosion under ground level on the outside.
: Which metod should i prefer?




 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
07:03 Jun-15-2000
Re: Inspection of lamppost`s
de surface clean and free of debris?

How much surface prep can be done?

If you can get your hand in to the inside surface I would suggest manual UT depending on the surface condition (call your local NDT service company)...or try the Panametrics Epoch 3 B-scan unit if you need a hard copy of the results with a linear digital output. (excellent unit for gathering thickness data for anticipated failure modeling)
;)




 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
09:44 Jun-15-2000
Re: Inspection of lamppost`s
Hi Johan,

We are currently working on this application in
consort with Dinsley Devices Ltd.

Assuming that the lamposts are manufactured from
tubular steel, and are fitted with the usual
electrical access door a few feet above the ground,
we can detect external corrosion well below ground
level, from the inside of the post.

We still have more work to do, but if you are
interested then please contact me by email.



 
 Reply 
 
Michael H. Dalichow
Michael H. Dalichow
00:53 Jun-15-2000
Re: Inspection of lamppost`s
Fraunhofer-IZFP in Saarbruecken, Germany, has developed a tool to inspect lamp posts from the above ground OD. The LIMAtest tool is based on EMAT technology licensed to ZWP Anlagenrevision GmbH in Germany.

Please contact ZWP by email at zwpar@zwpar.de; you can also check their english web sites at http://www.zwpar.de/index_uk.htm.

If you need further help please email me at mhd@qnetworld.com.

Good luck, Michael




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:29 Jun-15-2000
Re: Inspection of lamppost`s
This appears to be topic of the year around the world. We have completed a project assessing technologies for this application in both Europe and the Middle East. Some of the techniques you have already had replies from. If this is soil/air interface attack as a number of other people have experienced there are a number of techniques that do work without excavation.

The problem is not usually just one of inspection but also speed of inspection as highway lanes need to be closed and also varying geometries of lamp posts round, tapered, hexagonal.

The most effectibve method we have found which matches detection and assessment without excavation, along with data recording for verification (insurance audit considerations) and fast speed is Guided Wave Ultrasonics from GUL.

If you email me an address I can send you a copy of extracts from a study report.

Regards


 
 Reply 
 

Product Spotlight

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)

Download our white paper on Scatter Correction for Industrial Cone-Beam Computed Tomography (CBCT)
...
Using 3D VSHARP, a fast GPU-Based Linear Boltzmann Transport Equation Solver here: http://bit.ly/2Y0t78P
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window