Inspection of lamppost`s

I would like to inspect lamppost´s for corrosion under ground level on the outside.
Which metod should i prefer?


 
 Reply 
 
Joseph Pascente
Joseph Pascente
05:36 Jun-15-2000
Re: Inspection of lamppost`s

Lixi Profiler can make this measurement for wall
thickness on ourdoor lamp posts.


Regards,

Joe Pascente

: I would like to inspect lamppost´s for corrosion under ground level on the outside.
: Which metod should i prefer?




 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
07:03 Jun-15-2000
Re: Inspection of lamppost`s
de surface clean and free of debris?

How much surface prep can be done?

If you can get your hand in to the inside surface I would suggest manual UT depending on the surface condition (call your local NDT service company)...or try the Panametrics Epoch 3 B-scan unit if you need a hard copy of the results with a linear digital output. (excellent unit for gathering thickness data for anticipated failure modeling)
;)




 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
09:44 Jun-15-2000
Re: Inspection of lamppost`s
Hi Johan,

We are currently working on this application in
consort with Dinsley Devices Ltd.

Assuming that the lamposts are manufactured from
tubular steel, and are fitted with the usual
electrical access door a few feet above the ground,
we can detect external corrosion well below ground
level, from the inside of the post.

We still have more work to do, but if you are
interested then please contact me by email.



 
 Reply 
 
Michael H. Dalichow
Michael H. Dalichow
00:53 Jun-15-2000
Re: Inspection of lamppost`s
Fraunhofer-IZFP in Saarbruecken, Germany, has developed a tool to inspect lamp posts from the above ground OD. The LIMAtest tool is based on EMAT technology licensed to ZWP Anlagenrevision GmbH in Germany.

Please contact ZWP by email at zwpar@zwpar.de; you can also check their english web sites at http://www.zwpar.de/index_uk.htm.

If you need further help please email me at mhd@qnetworld.com.

Good luck, Michael




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:29 Jun-15-2000
Re: Inspection of lamppost`s
This appears to be topic of the year around the world. We have completed a project assessing technologies for this application in both Europe and the Middle East. Some of the techniques you have already had replies from. If this is soil/air interface attack as a number of other people have experienced there are a number of techniques that do work without excavation.

The problem is not usually just one of inspection but also speed of inspection as highway lanes need to be closed and also varying geometries of lamp posts round, tapered, hexagonal.

The most effectibve method we have found which matches detection and assessment without excavation, along with data recording for verification (insurance audit considerations) and fast speed is Guided Wave Ultrasonics from GUL.

If you email me an address I can send you a copy of extracts from a study report.

Regards


 
 Reply 
 

Product Spotlight

Conformable wedge transducer

The conformability is obtained with a flexible membrane filled with water between the transducer and
...
the inspected component. The coupling between the membrane and the component requires a small quantity of water or couplant. The conformable wedge combines the acoustic performance of immersion technique with good coupling and low attenuation.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window