Inspection of lamppost`s

I would like to inspect lamppost´s for corrosion under ground level on the outside.
Which metod should i prefer?


 
 Reply 
 
Joseph Pascente
Joseph Pascente
05:36 Jun-15-2000
Re: Inspection of lamppost`s

Lixi Profiler can make this measurement for wall
thickness on ourdoor lamp posts.


Regards,

Joe Pascente

: I would like to inspect lamppost´s for corrosion under ground level on the outside.
: Which metod should i prefer?




 
 Reply 
 
David Hermanutz
Consultant,
Hbndt.com, China, Joined Jul 2012, 85

David Hermanutz

Consultant,
Hbndt.com,
China,
Joined Jul 2012
85
07:03 Jun-15-2000
Re: Inspection of lamppost`s
de surface clean and free of debris?

How much surface prep can be done?

If you can get your hand in to the inside surface I would suggest manual UT depending on the surface condition (call your local NDT service company)...or try the Panametrics Epoch 3 B-scan unit if you need a hard copy of the results with a linear digital output. (excellent unit for gathering thickness data for anticipated failure modeling)
;)




 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
09:44 Jun-15-2000
Re: Inspection of lamppost`s
Hi Johan,

We are currently working on this application in
consort with Dinsley Devices Ltd.

Assuming that the lamposts are manufactured from
tubular steel, and are fitted with the usual
electrical access door a few feet above the ground,
we can detect external corrosion well below ground
level, from the inside of the post.

We still have more work to do, but if you are
interested then please contact me by email.



 
 Reply 
 
Michael H. Dalichow
Michael H. Dalichow
00:53 Jun-15-2000
Re: Inspection of lamppost`s
Fraunhofer-IZFP in Saarbruecken, Germany, has developed a tool to inspect lamp posts from the above ground OD. The LIMAtest tool is based on EMAT technology licensed to ZWP Anlagenrevision GmbH in Germany.

Please contact ZWP by email at zwpar@zwpar.de; you can also check their english web sites at http://www.zwpar.de/index_uk.htm.

If you need further help please email me at mhd@qnetworld.com.

Good luck, Michael




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:29 Jun-15-2000
Re: Inspection of lamppost`s
This appears to be topic of the year around the world. We have completed a project assessing technologies for this application in both Europe and the Middle East. Some of the techniques you have already had replies from. If this is soil/air interface attack as a number of other people have experienced there are a number of techniques that do work without excavation.

The problem is not usually just one of inspection but also speed of inspection as highway lanes need to be closed and also varying geometries of lamp posts round, tapered, hexagonal.

The most effectibve method we have found which matches detection and assessment without excavation, along with data recording for verification (insurance audit considerations) and fast speed is Guided Wave Ultrasonics from GUL.

If you email me an address I can send you a copy of extracts from a study report.

Regards


 
 Reply 
 

Product Spotlight

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window