07:22 Jun-23-2000
Low kv, pulsed x-ray source

We are hoping to use portable digital x-ray systems, such as those used to locate explosives in luggage, to find entrapped water in aircraft honeycomb structures.

The main problem is that these systems typically use the Golden Engineering 160kv pulsed source, which requires a lot of water in aluminum or composite skinned structures, to cast a shadow. Thus we are seeking much lower kv source, ideally 55 to 75kv.

We are aware that this is the range of medical and dental equipment, but thus far we have not located a stand-alone system that could be readily adapted to our needs.

Besides the above mentioned kilovolt range, we are looking for characteristics similar to that of the Golden Engineering System, that is, lightweight (< 10kg), and, ideally, relatively inexpensive and able to be battery-powered.

Any help would be appreciated.

Norm Woodward


 
 Reply 
 
John Pursley
R & D
Envision Product Design, USA, Joined Oct 1999, 23

John Pursley

R & D
Envision Product Design,
USA,
Joined Oct 1999
23
02:09 Jun-23-2000
Re: Low kv, pulsed x-ray source
: We are hoping to use portable digital x-ray systems, such as those used to locate explosives in luggage, to find entrapped water in aircraft honeycomb structures.

: The main problem is that these systems typically use the Golden Engineering 160kv pulsed source, which requires a lot of water in aluminum or composite skinned structures, to cast a shadow. Thus we are seeking much lower kv source, ideally 55 to 75kv.

: We are aware that this is the range of medical and dental equipment, but thus far we have not located a stand-alone system that could be readily adapted to our needs.

: Besides the above mentioned kilovolt range, we are looking for characteristics similar to that of the Golden Engineering System, that is, lightweight (< 10kg), and, ideally, relatively inexpensive and able to be battery-powered.

: Any help would be appreciated.

: Norm Woodward


Hi Norm,
The problem you describe with using the Golder Engineering pulse source has more to do with the imaging technology you are using than on the energy source.
Our latest digital X-ray system is completely battery operated and uses the Golden source to produce excellent (2-1T, >10 lp/mm) instant images from the thinest of materials up to .4" steel.
Click on http://DigitalRadioscopy.com for information on our Wearable X-ray Vision (tm) system.



 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
07:05 Jun-25-2000
Low kv, pulsed x-ray source
Dear Norm,

Please go to www.lixi.com for a low energy pulse
portable X-Ray.


Regards,

Lixi, Inc.


Joe Pascente


 
 Reply 
 
David Singer
David Singer
01:09 Jul-13-2000
Re: Low kv, pulsed x-ray source
: We are hoping to use portable digital x-ray systems, such as those used to locate explosives in luggage, to find entrapped water in aircraft honeycomb structures.

: The main problem is that these systems typically use the Golden Engineering 160kv pulsed source, which requires a lot of water in aluminum or composite skinned structures, to cast a shadow. Thus we are seeking much lower kv source, ideally 55 to 75kv.

: We are aware that this is the range of medical and dental equipment, but thus far we have not located a stand-alone system that could be readily adapted to our needs.

: Besides the above mentioned kilovolt range, we are looking for characteristics similar to that of the Golden Engineering System, that is, lightweight (< 10kg), and, ideally, relatively inexpensive and able to be battery-powered.

: Any help would be appreciated.

: Norm Woodward

I happen to know that Vidisco Ltd. of Israel have developed a real time system that has been approved by boeing and is being used by theIsrael Aircraft Industry for just this purpose. In fact, if I am not mistaken, they have an example image on their website. www.vidisco.com (If not then try .co.il.)
Happy to be of service.
David Singer


 
 Reply 
 
Sahýn Delýpýnar
Sahýn Delýpýnar
04:56 Nov-10-2000
Re: Low kv, pulsed x-ray source
: : We are hoping to use portable digital x-ray systems, such as those used to locate explosives in luggage, to find entrapped water in aircraft honeycomb structures.

: : The main problem is that these systems typically use the Golden Engineering 160kv pulsed source, which requires a lot of water in aluminum or composite skinned structures, to cast a shadow. Thus we are seeking much lower kv source, ideally 55 to 75kv.

: : We are aware that this is the range of medical and dental equipment, but thus far we have not located a stand-alone system that could be readily adapted to our needs.

: : Besides the above mentioned kilovolt range, we are looking for characteristics similar to that of the Golden Engineering System, that is, lightweight (< 10kg), and, ideally, relatively inexpensive and able to be battery-powered.

: : Any help would be appreciated.

: : Norm Woodward

: I happen to know that Vidisco Ltd. of Israel have developed a real time system that has been approved by boeing and is being used by the Israel Aircraft Industry for just this purpose. In fact, if I am not mistaken, they have an example image on their website. www.vidisco.com (If not then try .co.il.)
: Happy to be of service.
: David Singer




 
 Reply 
 
John Pursley
R & D
Envision Product Design, USA, Joined Oct 1999, 23

John Pursley

R & D
Envision Product Design,
USA,
Joined Oct 1999
23
00:33 Nov-10-2000
Re: Low kv, pulsed x-ray source
: : We are hoping to use portable digital x-ray systems, such as those used to locate explosives in luggage, to find entrapped water in aircraft honeycomb structures.

: : The main problem is that these systems typically use the Golden Engineering 160kv pulsed source, which requires a lot of water in aluminum or composite skinned structures, to cast a shadow. Thus we are seeking much lower kv source, ideally 55 to 75kv.

: : We are aware that this is the range of medical and dental equipment, but thus far we have not located a stand-alone system that could be readily adapted to our needs.

: : Besides the above mentioned kilovolt range, we are looking for characteristics similar to that of the Golden Engineering System, that is, lightweight (< 10kg), and, ideally, relatively inexpensive and able to be battery-powered.

: : Any help would be appreciated.

: : Norm Woodward


We now have an 80 Kev / 3 ma X-ray source that is small, battery operated, and light weight. See us at the ASNT conference in Indianapolis booth 328, or call 907-563-1141.



 
 Reply 
 
Patrick Doty
Patrick Doty
06:34 Oct-18-2001
Re: Low kv, pulsed x-ray source
: We are hoping to use portable digital x-ray systems, such as those used to locate explosives in luggage, to find entrapped water in aircraft honeycomb structures.

: The main problem is that these systems typically use the Golden Engineering 160kv pulsed source, which requires a lot of water in aluminum or composite skinned structures, to cast a shadow. Thus we are seeking much lower kv source, ideally 55 to 75kv.

: We are aware that this is the range of medical and dental equipment, but thus far we have not located a stand-alone system that could be readily adapted to our needs.

: Besides the above mentioned kilovolt range, we are looking for characteristics similar to that of the Golden Engineering System, that is, lightweight (< 10kg), and, ideally, relatively inexpensive and able to be battery-powered.

: Any help would be appreciated.

: Norm Woodward

Nuetron radiography is excells for imaging water in aircraft structures. There is a facility (currently under utilized) dedicated to this at the former McClellan AFB in Sacremento.


 
 Reply 
 

Product Spotlight

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window