Thin Gauge Steel Tubes

I am looking for a reliable way to UT thin gauge, under 5/16", steel tube that has a circumferential joint joined utilizing a backing bar.


 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
09:30 Jun-23-2000
Re: Thin Gauge Steel Tubes
: I am looking for a reliable way to UT thin gauge, under 5/16", steel tube that has a circumferential joint joined utilizing a backing bar.

I'm not sure I'm properly visualizing what you're doing, but if it's a brazed or welded joint, we may be able to do something with small diameter, sharply focussed immersion transducers and appropriate fixturing. The tube diameter itself is not a problem. If it's just mechanically clamped, on the other hand, it's not a good application for ultrasonic flaw detection.

I'd be happy to look at a drawing if you can send one.

--Tom Nelligan
Panametrics, Inc.




 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
07:02 Jun-25-2000
Re: Thin Gauge Steel Tubes
Dear Tom,

Go to www.lixi.com and then to Profiler. This non
contact wall thickness gauge will measure the wall
thickness of thin gauge steel tubes.


Regards,

Lixi, Inc.


Joe Pascente


 
 Reply 
 
Rick Pfannenstiel
Consultant
Spin LLC, USA, Joined Jun 2000, 1

Rick Pfannenstiel

Consultant
Spin LLC,
USA,
Joined Jun 2000
1
04:14 Jun-29-2000
Re: Thin Gauge Steel Tubes
We have been inspecting buttwelds in .056"T by 1.0" diameter buttwelds in inconnel tubing with great success using FAST ultrasonics. The backing ring should not be a problem. Not sure that this application is close to what you are doing. If you would like more information please email me.


 
 Reply 
 
Alexander Tsankov
Alexander Tsankov
01:17 Aug-03-2000
Carbon Steel Tubes
Dear Sirs,
I am interested in Carbon Steel Tubes with diameter 40-48mm. If you can help me please send me Reply on my e-mail: powercom@netbg.com.

Sincerelly Yours
A. Tsankov


 
 Reply 
 

Product Spotlight

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window