PT Marker

Does anyone know of a marker (preferably pencil) which will fluoresce and is low in sulpher? We have tried the high purity felt tipped markers but: #1 they don't fluoresce, #2 if the tip is depressed a bit too long they create quite a mess and #3 the ink comes off the part too readily with solvent when checking indications. Any information will be much appreciated.

Andrea Steen
NDT Engineer/Level III
Rolls-Royce Corporation


 
 Reply 
 
Andrea Steen
, Joined ,
06:17 Jun-28-2000
Re: PT Marker

: Does anyone know of a marker (preferably pencil) which will fluoresce and is low in sulphur? We have tried the high purity felt tipped markers but: #1 they don't fluoresce, #2 if the tip is depressed a bit too long they create quite a mess and #3 the ink comes off the part too readily with solvent when checking indications. Any information will be much appreciated.

: Andrea Steen
: NDT Engineer/Level III
: Rolls-Royce Corporation

After discussing this with my co-workers, we would also be satisfied if we could find a marker (pencil) which would be low in sulfur and stay on a part in the presence of a solvent. We can live without the fluorescence.


 
 Reply 
 
Dent McIntyre
Consultant, NDE Manager NDELevel III/3
NDT Consultant, Canada, Joined Nov 1998, 252

Dent McIntyre

Consultant, NDE Manager NDELevel III/3
NDT Consultant,
Canada,
Joined Nov 1998
252
06:29 Jun-28-2000
Re: PT Marker
We use a Markal Paint stick with the end sharpened with a knife and use it to mark underwater when doing a UT immersion test. When you remove it from the water the paint dries and will remain.
This might work for your application.

Does anyone know of a marker (preferably pencil) which will fluoresce and is low in sulphur? We have tried the high purity felt tipped markers but: #1 they don't fluoresce, #2 if the tip is depressed a bit too long they create quite a mess and #3 the ink comes off the part too readily with solvent when checking indications. Any information will be much appreciated.

: : Andrea Steen
: : NDT Engineer/Level III
: : Rolls-Royce Corporation

: After discussing this with my co-workers, we would also be satisfied if we could find a marker (pencil) which would be low in sulfur and stay on a part in the presence of a solvent. We can live without the fluorescence.




 
 Reply 
 
Thomas Murphy
NDT Inspector
USA, Joined Jul 2000, 16

Thomas Murphy

NDT Inspector
USA,
Joined Jul 2000
16
03:10 Jul-25-2000
Re: PT Marker
Hello,

We use a red Berol 165T china marker. It fluoresces and is not readily removed by de-natured alcohol. It can readily be removed with mineral spirits. It is one of the approved markers for pre-service inspection of compressor components in a combustion turbine. However, I cannot attest to the Sulfur content.

Regards,
Tom

: We use a Markal Paint stick with the end sharpened with a knife and use it to mark underwater when doing a UT immersion test. When you remove it from the water the paint dries and will remain.
: This might work for your application.

: Does anyone know of a marker (preferably pencil) which will fluoresce and is low in sulphur? We have tried the high purity felt tipped markers but: #1 they don't fluoresce, #2 if the tip is depressed a bit too long they create quite a mess and #3 the ink comes off the part too readily with solvent when checking indications. Any information will be much appreciated.

: : : Andrea Steen
: : : NDT Engineer/Level III
: : : Rolls-Royce Corporation

: : After discussing this with my co-workers, we would also be satisfied if we could find a marker (pencil) which would be low in sulfur and stay on a part in the presence of a solvent. We can live without the fluorescence.




 
 Reply 
 
dave ronson
dave ronson
07:16 Nov-06-2000
Re: PT Marker
: Hello,

: We use a red Berol 165T china marker. It fluoresces and is not readily removed by de-ntured alcohol. It can readily be removed with mineral spirits. It is one of the approved markers for pre-service inspection of compressor components in a combustion turbine. However, I cannot attest to the Sulfur content.

: Regards,
: Tom

: : We use a Markal Paint stick with the end sharpened with a knife and use it to mark underwater when doing a UT immersion test. When you remove it from the water the paint dries and will remain.
: : This might work for your application.

: : Does anyone know of a marker (preferably pencil) which will fluoresce and is low in sulphur? We have tried the high purity felt tipped markers but: #1 they don't fluoresce, #2 if the tip is depressed a bit too long they create quite a mess and #3 the ink comes off the part too readily with solvent when checking indications. Any information will be much appreciated.

: : : : Andrea Steen
: : : : NDT Engineer/Level III
: : : : Rolls-Royce Corporation

: : : After discussing this with my co-workers, we would also be satisfied if we could find a marker (pencil) which would be low in sulfur and stay on a part in the presence of a solvent. We can live without the fluorescence.

We have found Sanford Corp. #02435 Orange pencilworks great for FPI and MPI.



 
 Reply 
 

Product Spotlight

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Ultrasonic Squirter/Gantry System

TecScan’s NDT Ultrasonic Gantry Systems are industrial Squirter scanners designed for non-destru
...
ctive quality testing and raster scanning of large structures and parts. The Gantry Systems are usually composed of an Industrial Mechanical Scanner and a Control Room with System Workstation.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window