Many Holes Inspection Problem

We need an inspection method to look fo scores inside 5/8" diameter holes. The holes are in plates about 2" thick and the scores are along the length of the hole.
Does not sound too tough yet does it?

The crunch is there are 16000 + holes on each plate and there are over 50 plates.

Current method is manual hole by hole with back lighting.
We have tried a video camera that actually shows the scores holes quite well but the lighting can make a bad hole look good.
We have contacted the "Vision Technical types" but they say we cannot recognize these scores with their systems.

Does anyone have any ideas?




 
 Reply 
 
Trevor Easton
Engineering
Dofasco Inc, Canada, Joined Nov 1998, 13

Trevor Easton

Engineering
Dofasco Inc,
Canada,
Joined Nov 1998
13
09:21 Jul-12-2000
Re: Many Holes Inspection Problem
: We need an inspection method to look fo scores inside 5/8" diameter holes. The holes are in plates about 2" thick and the scores are along the length of the hole.

Are the scores along the full length of each hole?
A plug gauge incorporating a rotating surface measurement stylus may provide a means to recognize such a score.

You will still have to position the gauge manually unless it can be done as part of the machining process when the holes are formed.

Can you shed a little more light on the problem. Is this plate in a fixed location? What is it? Where is it?


 
 Reply 
 
Dent McIntyre
Consultant, NDE Manager NDELevel III/3
NDT Consultant, Canada, Joined Nov 1998, 252

Dent McIntyre

Consultant, NDE Manager NDELevel III/3
NDT Consultant,
Canada,
Joined Nov 1998
252
01:44 Jul-12-2000
Re: Many Holes Inspection Problem
: : We need an inspection method to look fo scores inside 5/8" diameter holes. The holes are in plates about 2" thick and the scores are along the length of the hole.

: Are the scores along the full length of each hole?

NO. The scores may start and Stop within the hole. They are caused by the broaching operation. The scores are actually on the 3 lands that are formed by the broaching process.
: A plug gauge incorporating a rotating surface measurement stylus may provide a means to recognize such a score.

: You will still have to position the gauge manually unless it can be done as part of the machining process when the holes are formed.

: Can you shed a little more light on the problem. Is this plate in a fixed location? What is it? Where is it?

The plates are all loose and are in a manufacturing shop. They are about 10' diameter




 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
02:35 Jul-12-2000
Re: Many Holes Inspection Problem
How unsophisticated do you want to be ?

I remember about 20 years ago having a similar problem during broaching of gearbox components. We played with surface profiling, eddy current etc.

As in the end all we wanted to do was identify good and bad we went for cheap and cheerful. Lay the plates against a solid backing pour molten wax into each hole (as is used in wax casting process) leave to cool. Push out and look for the gooving on the wax slug, mark off good versus bad holes. You can probably do a pour of 500-600 holes in30 minutes, push out and inspect one hole every 3 minutes. Wax slugs you recycle back into the melt.

Regards

John O'Brien



 
 Reply 
 
James Doyle
James Doyle
02:16 Jul-21-2000
Re: Many Holes Inspection Problem
: We need an inspection method to look fo scores inside 5/8" diameter holes. The holes are in plates about 2" thick and the scores are along the length of the hole.
: Does not sound too tough yet does it?

: The crunch is there are 16000 + holes on each plate and there are over 50 plates.

: Current method is manual hole by hole with back lighting.
: We have tried a video camera that actually shows the scores holes quite well but the lighting can make a bad hole look good.
: We have contacted the "Vision Technical types" but they say we cannot recognize these scores with their systems.

: Does anyone have any ideas?

: Dent,
This may be too expensive - but we make non-contact, laser-based scanners. They can generate a profile image as well as a video-like image. We find that scratches and score marks tend to show up very well with the video image. This is not a bore scope devise.
Check out our web site www.visualogic.com

If this will be an ongoing process the probe could be positioned like a drill tool and rapidly run in-and-out of each hole.

Good luck,

Jim Doyle





 
 Reply 
 

Product Spotlight

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window