Technical Discussions
Torbjorn Lofqvist
Torbjorn Lofqvist
04:04 Apr-15-1999
Kramers-Kronig relation?

Hi all!

I am a PhD student studying the acoustics of fibre suspensions.
I work at Lulea Univ. of Tech., Sweden, and have a question for
you.
Could someone give me a good reference for the basis of
the Kramers-Kronig relationship?

Greateful for all suggestions!

--Torbjorn


 
 Reply 
 
M. Schickert
R & D,
Institute for Materials Research and Testing, Germany, Joined Jan 2000, 18

M. Schickert

R & D,
Institute for Materials Research and Testing,
Germany,
Joined Jan 2000
18
06:50 Apr-15-1999
Re: Kramers-Kronig relation?
: Hi all!

: I am a PhD student studying the acoustics of fibre suspensions.
: I work at Lulea Univ. of Tech., Sweden, and have a question for
: you.
: Could someone give me a good reference for the basis of
: the Kramers-Kronig relationship?

Dear Torbjorn,

This one is the basis - as you inquired:
R. de L. Kronig: "On the theory of dispersion of x-rays".
J. Opt. Soc. Am. 12 (1926) 547-557

This one is from Stockholm - more related to ultrasound:
J.L. Leander: "On the relation between the wavefront speed and
the group velocity concept".
J. Acoust. Soc. Am. 100 (1996) 3503-3507.

Sincerely, Martin

Materials Research and Testing Institute
at the Bauhaus-University Weimar, Germany



 
 Reply 
 
Silvio Kruger
Silvio Kruger
08:52 Apr-22-1999
Re: Kramers-Kronig relation?
: Hi all!

: I am a PhD student studying the acoustics of fibre suspensions.
: I work at Lulea Univ. of Tech., Sweden, and have a question for
: you.
: Could someone give me a good reference for the basis of
: the Kramers-Kronig relationship?

: Greateful for all suggestions!

: --Torbjorn

Some references for ultrasonics are:
Ye, Z; Acoustic Dispersion and Attenuation in many
Spherial Scatterers Systems and the Kramers-Kronig
Relations; Journal of the Acoustic Society of America
101 (6) 1997; pp.3299-3305

Szabo, T. L.; Causal Theories and Data for Acoustic
Attenuation Obeying a Frequency Power Law;
Journal of the Acoustic Society of America; 97(1);
1995; pp.14-24

O'Donnell, M.;Jaynes, E. T.; Miller, J. G.;
Kramers-Kronig Relationship Between Ultrasonic
Attenuation and Phase Velocity; Journal of the
Acoustic Society of America; 69(3) 1981; pp.696-701

O'DONELL, M.; JAYNES, E. T.; MILLER, J. G.
"General Relationship Between Ultrasonic Attenuation
and Dispesion" Journal of the Acoustical Society
of America,63(6) 1978, pp.1935-1937.

You can e-mail me for discussions.
Silvio Kruger




 
 Reply 
 
Ricardo González
Ricardo González
02:24 Jul-18-2000
Kramers-Kronig program
How I get a Kramers-Kronig Relations Fortran program?



 
 Reply 
 
ouaheb
ouaheb
05:57 Nov-26-2000
Re: Kramers-Kronig program
: How I get a Kramers-Kronig Relations Fortran program?




 
 Reply 
 
Alexey Kochura
Alexey Kochura
00:17 Nov-16-2001
Re: Kramers-Kronig program
: How I get a Kramers-Kronig Relations Fortran program?
Alexey Kochura




 
 Reply 
 
eiad alberto
eiad alberto
03:42 Dec-31-2001
Re: Kramers-Kronig relation?
: : Hi iwant information about optical properties and excition of cry




 
 Reply 
 
Adelmo Freire
Adelmo Freire
06:30 Jul-30-2002
Re: Kramers-Kronig program
I wold appreciate a lot a Kramers-Kronig Relations MATLAB/FORTRAN program? Thanks. Adelmo Freire.



 
 Reply 
 

Product Spotlight

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Surf-X® Array Probe

Introducing the Surf-X family of flexible Eddy Current Array (ECA) probes. Featuring unique multiple
...
coil sets and proprietary X-PROBE technology, Surf-X array probes can quickly and accurately handle a range of inspection applications, from inspecting corrosion or cracking in pipes, pressure vessels, or tanks, to assessing and sizing cracks in raised welds and friction stir welds.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window