11,650 mm tube inspection

We have been asked to perform a test of tubes of 11,650 mm (0,4") diameters.
Has anyone experienced this kind of test with IRIS and/or RFT ?
Do so small probes exist ?

Thank you.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
03:31 Jul-21-2000
11.650 mm tube inspection
Dear Amedeo,

The Lixi Profiler can measure the total wall thickness of tubes whose diameter is less than 1mm. Your request was for tubing 11,650mm which mean 11.650mm. Sorry that I am not use to using a comma instead of a period.


Regards,

Joe Pascente


 
 Reply 
 
Frederick Beck
Frederick Beck
07:16 Jul-21-2000
Re: 11.650 mm tube inspection

: Dear Amedeo,

: The Lixi Profiler can measure the total wall thickness of tubes whose diameter is less than 1mm. Your request was for tubing 11,650mm which mean 11.650mm. Sorry that I am not use to using a comma instead of a period.

:
: Regards,

: Joe Pascente

Tac Technical Instrument corp in Trenton, NJ USA specializes in ultrasonic tubing inspection systems. There are a number of transducers suitable for inspection of tubes with the diameter and wall thickness you mention. Please contact us for more information



 
 Reply 
 
Andre van Vuuren
Andre van Vuuren
01:19 Jul-21-2000
Re: 11,650 mm tube inspection
No info on wall thickness or tube material?
There is a micro turbine available for the IRIS System. This can inspect tubing down to +/- 8.5mm internal ID. Used with great results with the TC5700. The smallest RFT probe we use is a 10.5MM probe available from RDtech.


 
 Reply 
 
James Doyle
James Doyle
02:05 Jul-21-2000
Re: 11,650 mm tube inspection
: We have been asked to perform a test of tubes of 11,650 mm (0,4") diameters.
: Has anyone experienced this kind of test with IRIS and/or RFT ?
: Do so small probes exist ?

: Thank you.

We have developed a laser-based tube inspection system that will operate in tubes to about 6.5 mm ID (0.260-ich)
The probe operates in straight tubes and the software generates a nice cross-sectional and "C"-scan image. You can check it out at www.visualogic.com

Jim Doyle


 
 Reply 
 
Wieslaw Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 276

Wieslaw Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
276
05:47 Jul-22-2000
Re: 11,650 mm tube inspection
: We have been asked to perform a test of tubes of 11,650 mm (0,4") diameters.
: Has anyone experienced this kind of test with IRIS and/or RFT ?
: Do so small probes exist ?

: Thank you.

We can make ultrasonic probes with about 3mm diameter and very short pulse (about 50ns long, 20MHz medium frequency).

It is also possible to make such probes with transducer radiating in 90 degrees to the axe of the probe. You can find more information about our transducer on the following site:
http://www.optel.com.pl/manual/english/transd.htm

Wieslaw Bicz

Optel sp. z o.o.



 
 Reply 
 
Ingo Becker
Engineering, NDT Inspector & Sales
ec-works GmbH, Germany, Joined Apr 2000, 31

Ingo Becker

Engineering, NDT Inspector & Sales
ec-works GmbH,
Germany,
Joined Apr 2000
31
02:47 Jul-25-2000
Re: 11,650 mm tube inspection
Hello Amadeo,

why not testing the tubes (how many?) with eddy current technology? The diameter of 11.65 mm (inside/outside?) is not a problem, we have even smaller probes in stock. Please tell us something about the tube material, metal? Which?

For further information contact us or visit our exhibition or homepage www.deltatest.de

regards


ingo becker


 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

GUL Subsea Solutions - Screeening & Monitoring

To inspect new and existing subsea lines, you need proven technology and experience. GUL offers it's
...
technology to solve this challenge: GUL Subsea and gMAT Transducer Rings.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window