00:35 Jul-21-2000
11,650 mm tube inspection

We have been asked to perform a test of tubes of 11,650 mm (0,4") diameters.
Has anyone experienced this kind of test with IRIS and/or RFT ?
Do so small probes exist ?

Thank you.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
03:31 Jul-21-2000
11.650 mm tube inspection
Dear Amedeo,

The Lixi Profiler can measure the total wall thickness of tubes whose diameter is less than 1mm. Your request was for tubing 11,650mm which mean 11.650mm. Sorry that I am not use to using a comma instead of a period.


Regards,

Joe Pascente


 
 Reply 
 
Frederick Beck
Frederick Beck
07:16 Jul-21-2000
Re: 11.650 mm tube inspection

: Dear Amedeo,

: The Lixi Profiler can measure the total wall thickness of tubes whose diameter is less than 1mm. Your request was for tubing 11,650mm which mean 11.650mm. Sorry that I am not use to using a comma instead of a period.

:
: Regards,

: Joe Pascente

Tac Technical Instrument corp in Trenton, NJ USA specializes in ultrasonic tubing inspection systems. There are a number of transducers suitable for inspection of tubes with the diameter and wall thickness you mention. Please contact us for more information



 
 Reply 
 
Andre van Vuuren
Andre van Vuuren
01:19 Jul-21-2000
Re: 11,650 mm tube inspection
No info on wall thickness or tube material?
There is a micro turbine available for the IRIS System. This can inspect tubing down to +/- 8.5mm internal ID. Used with great results with the TC5700. The smallest RFT probe we use is a 10.5MM probe available from RDtech.


 
 Reply 
 
James Doyle
James Doyle
02:05 Jul-21-2000
Re: 11,650 mm tube inspection
: We have been asked to perform a test of tubes of 11,650 mm (0,4") diameters.
: Has anyone experienced this kind of test with IRIS and/or RFT ?
: Do so small probes exist ?

: Thank you.

We have developed a laser-based tube inspection system that will operate in tubes to about 6.5 mm ID (0.260-ich)
The probe operates in straight tubes and the software generates a nice cross-sectional and "C"-scan image. You can check it out at www.visualogic.com

Jim Doyle


 
 Reply 
 
Wieslaw Bicz
Engineering,
PBP Optel sp. z o.o., Poland, Joined Feb 2009, 276

Wieslaw Bicz

Engineering,
PBP Optel sp. z o.o.,
Poland,
Joined Feb 2009
276
05:47 Jul-22-2000
Re: 11,650 mm tube inspection
: We have been asked to perform a test of tubes of 11,650 mm (0,4") diameters.
: Has anyone experienced this kind of test with IRIS and/or RFT ?
: Do so small probes exist ?

: Thank you.

We can make ultrasonic probes with about 3mm diameter and very short pulse (about 50ns long, 20MHz medium frequency).

It is also possible to make such probes with transducer radiating in 90 degrees to the axe of the probe. You can find more information about our transducer on the following site:
http://www.optel.com.pl/manual/english/transd.htm

Wieslaw Bicz

Optel sp. z o.o.



 
 Reply 
 
Ingo Becker
Engineering, NDT Inspector & Sales
ec-works GmbH, Germany, Joined Apr 2000, 31

Ingo Becker

Engineering, NDT Inspector & Sales
ec-works GmbH,
Germany,
Joined Apr 2000
31
02:47 Jul-25-2000
Re: 11,650 mm tube inspection
Hello Amadeo,

why not testing the tubes (how many?) with eddy current technology? The diameter of 11.65 mm (inside/outside?) is not a problem, we have even smaller probes in stock. Please tell us something about the tube material, metal? Which?

For further information contact us or visit our exhibition or homepage www.deltatest.de

regards


ingo becker


 
 Reply 
 

Product Spotlight

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window