03:28 Jul-31-2000
Penetrant Testing

I have few questions regarding Penetrant Testing,

1. What is the nature of Penetrant and Developer, i.e.,whether
they are acid or base
2. What is the suitable cleaning method for dry developers?
3. Preheating the Penetrant/Specimen is recommended or not, what
is the effect of preheating?
4. What is the relationship between Dragoutloss and viscosity
5. How the rate of penetration is related to Viscosity, Specific
gravity and surface tension
6. What method shall be employed to inspect out side weld of
open ethelene storage tank
7. What is the suitable cleaning method for metals, rusted and
scaled surfaces
If any one knows the correct answer, please send you email

by
N.Kuppusamy


 
 Reply 
 
Suman dey
Suman dey
07:06 Dec-31-2000
Re: Penetrant Testing
Could u please help me to understand te relation between surface tension and penetration

Regards
Suman Dey


 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

Ultrasonic tomograph for imaging of concrete structures А1040 MIRA

Applicable for concrete inspection allowing imaging of the internal structure of objects from conc
...
rete, reinforced concrete, different stones. The operation applies pulse-echo technique at one-side access to the object. The instrument is feasible for concrete inspection for searching conduct ducts, conduits, detection of foreign inclusions, holes, honeycombing, cracks and other concrete defects.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window