about austenitic steel ndt

where can I get some information about austenitic steel NDT, especially on electric generator, whose material is 50Mn18Cr4WN(18MnCr4)?
thank you for your help.


 
 Reply 
 
nard
nard
07:49 Aug-05-2000
Re: about austenitic steel ndt
Dear A.Delahaza
We have over 30 years experience in the examination of austenitic steel
welds . Special longitudinal angled probe have to be used to penetrate the
austenitc colonnar structure . Actually we are in Korea to train people for
the examination pressure vessels with heavy thicknesses .At the 15 World
Conference on NDT we will present a paper on this subject .
Send me you fax number , will send you material .
I&T NARDONI INSTITUTE nardoni @numerica.it Brescia Italy fax
0039 -030-2667429 .
Handy phone :
0039-348-2280470


best regards


G:NARDONI


----------
: where can I get some information about austenitic steel NDT, especially on electric generator, whose material is 50Mn18Cr4WN(18MnCr4)?
: thank you for your help.




 
 Reply 
 
Thomas Murphy
NDT Inspector
USA, Joined Jul 2000, 16

Thomas Murphy

NDT Inspector
USA,
Joined Jul 2000
16
07:31 Aug-07-2000
Re: about austenitic steel ndt
EPRI (Electrical Power Research Institute)
In Charlotte, South Carolina, USA has published an
exhaustive recomendation manual for this exact
application. The retaining rings are difficult to
inspect. Inspection methods are similar to those
employed during inspection of austentic piping
but are different enough that specialized training
would be recommended for a new inspector. The EPRI
report lists both the inspection possibilities (UT,
ET, PT, VT) as well as the advantages and disadvantages
of each. It also touches on the fracture mechanics,
flaw types, and methods of repair. The report number
is EPRI EL/EM-5117-SR it can also be accessed by the
topics of retaining rings, stress corrosion cracking,
nondestructive testing and in-service inspection.

Regards,
Tom

: where can I get some information about austenitic steel NDT, especially on electric generator, whose material is 50Mn18Cr4WN(18MnCr4)?
: thank you for your help.




 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>