09:48 Aug-06-2000
creeping wave

dear sirs
for the past year i have been playing with id and od creeping wave probes.
i have now made a probe with a polarized shoe that creeps on the id and the od at the same time.
can anyone tell me what to do with it.





 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
03:31 Aug-07-2000
Re: creeping wave



 
 Reply 
 
J. Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J. Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
03:38 Aug-07-2000
Re: creeping wave



 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1300

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1300
02:14 Aug-07-2000
Re: creeping wave
Andy:
I would be interested to learn more about the "polarisation shoe".
The "so-called" creeping wave is putatively formed as a result of a simple compression wave interacting at a free boundary.
Upon incidence from the shoe designed to provide a refracted angle somewhere between about 70-80 degrees in the solid test piece, the "creeping wave" forms on the near surface.
Since the incident angle from the shoe ALSO results in an SV shear mode at a smaller angle (typically 30-35 degrees) a second mode conversion occurs on the far surface (assuming it to be parallel to the near surface).
The mode converted wave is of course compression (converted from SV Shear). The angle of the converted compression wave off the far surface is similar to the initial refracted angle (between 70-80 degrees) and the same mechanics account for the initiation of the far surface "creeping wave".

These principles are well explained in a paper on dissimilar metals by Dr. Schmid (you can find it in a back issueof the NDT.net).

My point is that the Near and Far (ID and OD) creeping waves are a naturally occuring event but they could not occur at the "same" time. The near (OD?) occurs first and the far (ID?) occurs after the slower SV shear wave has impinged on the far surface.

If you meant that your probe can produce both I think you could have achieved the same results with a 70 degree L Wave probe.

Ed


: dear sirs
: for the past year i have been playing with id and od creeping wave probes.
: i have now made a probe with a polarized shoe that creeps on the id and the od at the same time.
: can anyone tell me what to do with it.





 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window