x-ray film processors

Does anyone have information on GE aquiring Agfa? Need to know if the money would be well spent on agfa's tradition x-ray processing equipment. What are GE's plans for NDT in this area?


    
 
 
Ralph
Ralph
05:49 Feb-25-2004
Re: x-ray film processors
----------- Start Original Message -----------
: Does anyone have information on GE aquiring Agfa? Need to know if the money would be well spent on agfa's tradition x-ray processing equipment. What are GE's plans for NDT in this area?
------------ End Original Message ------------
GE seems to be activly selling film, processors and parts for the AGFA NDT processors. I work with them everyday. Go for it!




    
 
 
Scott Longstreet
Scott Longstreet
02:48 Feb-25-2004
Re: x-ray film processors
----------- Start Original Message -----------
: : Does anyone have information on GE aquiring Agfa? Need to know if the money would be well spent on agfa's tradition x-ray processing equipment. What are GE's plans for NDT in this area?
: GE seems to be activly selling film, processors and parts for the AGFA NDT processors. I work with them everyday. Go for it!
------------ End Original Message ------------
I use all Agfa products. Film, Solutions and a NDT-E film processor.The processor has infrared drying,a water saving feature and produces blemish free film!




    
 
 
Fred Raco, Jr.
Consultant,
RNDT, Inc., USA, Joined Jul 2002, 24

Fred Raco, Jr.

Consultant,
RNDT, Inc.,
USA,
Joined Jul 2002
24
04:07 Feb-26-2004
Re: x-ray film processors
----------- Start Original Message -----------
: : : Does anyone have information on GE aquiring Agfa? Need to know if the money would be well spent on agfa's tradition x-ray processing equipment. What are GE's plans for NDT in this area?
: : GE seems to be activly selling film, processors and parts for the AGFA NDT processors. I work with them everyday. Go for it!
: I use all Agfa products. Film, Solutions and a NDT-E film processor.The processor has infrared drying,a water saving feature and produces blemish free film!
------------ End Original Message ------------

We have a Pantak/Seifert X-ray tube, Agfa processor, and use their chemistry and film. We couldn't have hooked up with a better company. We are important to them and they let us know that. Excellent "after the sale" service!


    
 
 
Dave Davies
Dave Davies
01:24 Feb-27-2004
Re: x-ray film processors
----------- Start Original Message -----------
: : : Does anyone have information on GE aquiring Agfa? Need to know if the money would be well spent on agfa's tradition x-ray processing equipment. What are GE's plans for NDT in this area?
: : GE seems to be activly selling film, processors and parts for the AGFA NDT processors. I work with them everyday. Go for it!
: I use all Agfa products. Film, Solutions and a NDT-E film processor.The processor has infrared drying,a water saving feature and produces blemish free film!
------------ End Original Message ------------


It is interesting that the replies to this query, so far, are all testimonials. I too am using an AGFA processor which is scheduled for replacement this year. I would like to replace with AGFA as we use their films and chemistry.
What about a direct reply from GE on their committment? This is a major purchase and will need support for some years, are GE and AGFA going to commit?
What about non film radiography, has anyone any information on it replacing conventional film for on site work e.g. radiography of 20 - 36 inch diameter piping up to 2 inches thick?


    
 
 
Fred Raco, Jr.
Consultant,
RNDT, Inc., USA, Joined Jul 2002, 24

Fred Raco, Jr.

Consultant,
RNDT, Inc.,
USA,
Joined Jul 2002
24
04:02 Feb-27-2004
Re: x-ray film processors
----------- Start Original Message -----------
: : : : Does anyone have information on GE aquiring Agfa? Need to know if the money would be well spent on agfa's tradition x-ray processing equipment. What are GE's plans for NDT in this area?
: : : GE seems to be activly selling film, processors and parts for the AGFA NDT processors. I work with them everyday. Go for it!
: : I use all Agfa products. Film, Solutions and a NDT-E film processor.The processor has infrared drying,a water saving feature and produces blemish free film!
:
: It is interesting that the replies to this query, so far, are all testimonials. I too am using an AGFA processor which is scheduled for replacement this year. I would like to replace with AGFA as we use their films and chemistry.
: What about a direct reply from GE on their committment? This is a major purchase and will need support for some years, are GE and AGFA going to commit?
: What about non film radiography, has anyone any information on it replacing conventional film for on site work e.g. radiography of 20 - 36 inch diameter piping up to 2 inches thick?
------------ End Original Message ------------

What specification are you shooting too? ASME V, Article 2, Appendix 4 will give you some information.



    
 
 

Product Spotlight

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

High Resolution Industrial CT System for Small/Medium Size Parts Inspection - YXLON FF35 CT

The YXLON FF35 CT computed tomography system is designed to achieve extremely precise inspection r
...
esults for a wide range of applications. Available in a single or dual tube configuration, it is perfect for very small to medium size parts inspection in the automotive, electronics, aviation, and material science industries.
>

TVC awarded UKAS accreditation

TVC are delighted to finally announce we have been awarded UKAS accreditation for our calibration
...
laboratory. Laboratory accreditation to ISO/IEC 17025:2005 enables us to conduct the Electrical Verification of Ultrasonic Flaw Detection Equipment to BS EN 12668-1:2010. It has taken many months of hard work and we want to thank our staff for all their efforts during this massive undertaking.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window