25 kV overhead hard drawn Copper Contact wire

We are facing the problem of unexplained breakage of contact wire
of 107 square millimeter ( one fourth of a square inch ) which is kept
under 1000 Kg ( 2240 pounds ) tension.
It carries current to electric locomotives through a Pantograph
which maintains 7 Kg pressure.
Any suggestions for preventive diagonostics and testing of contact
wire before stringing ?
Dinesh Bansal, Chennai ( Madras ) , India



 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 307

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
307
08:17 Jun-14-1999
Re: 25 kV overhead hard drawn Copper Contact wire
: We are facing the problem of unexplained breakage of contact wire
: of 107 square millimeter ( one fourth of a square inch ) which is kept
: under 1000 Kg ( 2240 pounds ) tension.
: It carries current to electric locomotives through a Pantograph
: which maintains 7 Kg pressure.
: Any suggestions for preventive diagonostics and testing of contact
: wire before stringing ?
: Dinesh Bansal, Chennai ( Madras ) , India
:

Hallo Mr. Bansal.
I suggest that the copper wire is eddy current tested before installing. Use this to detect cracks and splits in the wire, and also to detect local inhomogenieties in the wire.
Is the supplier in India or elsewhere in the world. You may be able to specify tested wire in yiour purchase.
The problem may also be caused by local arc burning of the wire from disconnections and recommections of the locomotives whilst in service.

Regards
Godfrey Hands



 
 Reply 
 
Siamak Shokri (Msc in metallurgical Engineering)
Siamak Shokri (Msc in metallurgical Engineering)
04:07 Aug-14-2000
Re: 25 kV overhead hard drawn Copper Contact wire
We are looking for production of grooved contact wire in Railways research center of Iran.We need some information about production of it.we will be glad if you send us this information or introduce us to suppliers of this type of wires.
our address is:
Iran Railways research center,production group
no.201 Italia crossing,Vessal avenue
Tehran,Iran
Fax no. 009821-651462
Yours Faithful



 
 Reply 
 

Product Spotlight

A1525 SOLO

A1525 Solo – the most compact and affordable TMF unit with two phased array transducers and 3D v
...
isualization and analysis software in standard delivery set. A compact, ergonomic and easy to handheld Phased Array unit based on Total Focusing Method for easy-going imaging of inspection objects with two-dimensional and three-dimensional visualization and evaluation of inspection results.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window