Use of Acoustics and Ultrasonics evaluating wood properties

I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.

I am looking for a nucleus of research comprising expertise and knowledge in both the areas of sonics and wood science and with a current, ongoing research program in this area and an interest in partnering with private industry in the USA.


 
 Reply 
 
Dr. Christian Grosse
Teacher,
Technische Universität München, Germany, Joined Nov 2000, 11

Dr. Christian Grosse

Teacher,
Technische Universität München,
Germany,
Joined Nov 2000
11
09:55 Dec-19-1998
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.

: I am looking for a nucleus of research comprising expertise and knowledge in both the areas of sonics and wood science and with a current, ongoing research program in this area and an interest in partnering with private industry in the USA.

There is a research project at the University of Stuttgart on the use of ultrasonics and acoustic emission in wood.
You can contact Dr. Simon Aicher at simon.aicher@po.uni-stuttgart.de




 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 609

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
609
02:39 Dec-21-1998
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.

: I am looking for a nucleus of research comprising expertise and knowledge in both the areas of sonics and wood science and with a current, ongoing research program in this area and an interest in partnering with private industry in the USA.
-----------

The Table of contents of the NDT of Wood Proceedings is available at
http://www.ndt.net/publicat/bibliog/cnflw_96.htm

The 10th International Symposium on Nondestructive Testing Lausanne
- Switzerland Aug 96.

This Symposium was organized by IBOIS - Chair of Timber Construction of the
Swiss Federal Institute of Technology in Lausanne, with Prof. Jean Luc Sandoz.

See the sample full-text at:
http://www.ndt.net//article/sandoz/sandoz.htm
Ultrasonic solid wood evaluation in industrial applications
by J. L. Sandoz



 
 Reply 
 
saeed kazemi
saeed kazemi
07:30 Dec-18-1999
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: : I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.

: : I am looking for a nucleus of research comprising expertise and knowledge in both the areas of sonics and wood science and with a current, ongoing research program in this area and an interest in partnering with private industry in the USA.
: -----------

: The Table of contents of the NDT of Wood Proceedings is available at
: http://www.ndt.net/publicat/bibliog/cnflw_96.htm

: The 10th International Symposium on Nondestructive Testing Lausanne
: - Switzerland Aug 96.

: This Symposium was organized by IBOIS - Chair of Timber Construction of the
: Swiss Federal Institute of Technology in Lausanne, with Prof. Jean Luc Sandoz.

: See the sample full-text at:
: http://www.ndt.net//article/sandoz/sandoz.htm
: Ultrasonic solid wood evaluation in industrial applications
: by J. L. Sandoz




 
 Reply 
 
emmet mcgauran
emmet mcgauran
07:20 Jul-06-2000
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: : I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.

: : I am looking for a nucleus of research comprising expertise and knowledge in both the areas of sonics and wood science and with a current, ongoing research program in this area and an interest in partnering with private industry in the USA.
: -----------

: The Table of contents of the NDT of Wood Proceedings is available at
: http://www.ndt.net/publicat/bibliog/cnflw_96.htm

: The 10th International Symposium on Nondestructive Testing Lausanne
: - Switzerland Aug 96.

: This Symposium was organized by IBOIS - Chair of Timber Construction of the
: Swiss Federal Institute of Technology in Lausanne, with Prof. Jean Luc Sandoz.

: See the sample full-text at:
: http://www.ndt.net//article/sandoz/sandoz.htm
: Ultrasonic solid wood evaluation in industrial applications
: by J. L. Sandoz




 
 Reply 
 
Antonio Pires Azevedo Júnior
Antonio Pires Azevedo Júnior
00:42 Sep-15-2000
Re: Use of Acoustics and Ultrasonics evaluating wood properties

: : : I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.

: : : I am looking for a nucleus of research comprising expertise and knowledge in both the areas of sonics and wood science and with a current, ongoing research program in this area and an interest in partnering with private industry in the USA.
: : -----------

: : The Table of contents of the NDT of Wood Proceedings is available at
: : http://www.ndt.net/publicat/bibliog/cnflw_96.htm

: : The 10th International Symposium on Nondestructive Testing Lausanne
: : - Switzerland Aug 96.

: : This Symposium was organized by IBOIS - Chair of Timber Construction of the
: : Swiss Federal Institute of Technology in Lausanne, with Prof. Jean Luc Sandoz.

: : See the sample full-text at:
: : http://www.ndt.net//article/sandoz/sandoz.htm
: : Ultrasonic solid wood evaluation in industrial applications
: : by J. L. Sandoz




 
 Reply 
 
R. H. Greene
R. H. Greene
00:13 Oct-19-2000
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: I am interested in any experimental results using propagated acoustic waves to penetrate wood of various species...wavelength transmission characteristics, etc.


 
 Reply 
 
Carmen Herrera
Carmen Herrera
00:14 Nov-29-2001
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: I am interested in finding out who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood and wood based panels.





 
 Reply 
 
Rodrigo Terezo
Rodrigo Terezo
00:49 Dec-23-2002
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: : I am interested in finding out articles and who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.



 
 Reply 
 
Pedro Feres Filho
Director,
Brazil, Joined Jul 2001, 1

Pedro Feres Filho

Director,
Brazil,
Joined Jul 2001
1
01:09 Dec-23-2002
Re: Use of Acoustics and Ultrasonics evaluating wood properties
: : : I am interested in finding out articles and who is currently doing research applying acoustic and ultrasonic testing techniques to understanding and evaluating the properties of wood, in particular, solid wood.
.
Dear Rodrigo, we have acoustic tecnology available for this application. Por favor entre em contato (11 3082 5111)


 
 Reply 
 

Product Spotlight

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

NovaScope 6000

The all-digital Novascope 6000 is a portable, ultra-high precision thickness gauge for high-speed
...
thickness measurement. Novascope 6000 has unmatched capabilities and unique features including: •Superior Resolution with high contrast, high-speed color RF display •High pulser voltage •Real-time video output •Increased internal/external data storage •Programmable SetUp features •Battery & AC Powered
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window