Phani
Phani
00:01 May-19-2005
Phased array Probes

Can any Please tell me the difference between the Phase array transducers and linear array transducers.
are they same or different?

Thanks
Phani


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 526

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
526
01:45 May-19-2005
Re: Phased array Probes
The simple answer is yes they are the same, but not exactly. An array of any shape is 'phased' by driving the different array elements with different timing, so that the resultant beam is scanned, steered or focused.

Most phased array transducers are linear arrays, but annular, segmented or 2-D arrays can also be driven by phased array equipment

Joe


---------- Start Original Message -----------
: Can any Please tell me the difference between the Phase array transducers and linear array transducers.
: are they same or different?
: Thanks
: Phani
------------ End Original Message ------------




 
 Reply 
 
Paul A. Meyer
R & D,
GE Inspection Technologies, USA, Joined Nov 1998, 47

Paul A. Meyer

R & D,
GE Inspection Technologies,
USA,
Joined Nov 1998
47
02:26 May-20-2005
Re: Phased array Probes
Because the sound field is steered or focused, as indicated in the previous response, the individual elements in the array must be designed properly so sound field will maintain its integrity over the intended phasing range. Older style linear arrays with large elements are not suitable for many phased applications. This is the reason many phased arrays appear smaller than non-phased designs.
I hope this helps.
Paul

----------- Start Original Message -----------
: The simple answer is yes they are the same, but not exactly. An array of any shape is 'phased' by driving the different array elements with different timing, so that the resultant beam is scanned, steered or focused.
: Most phased array transducers are linear arrays, but annular, segmented or 2-D arrays can also be driven by phased array equipment
: Joe
:
: ---------- Start Original Message -----------
: : Can any Please tell me the difference between the Phase array transducers and linear array transducers.
: : are they same or different?
: : Thanks
: : Phani
------------ End Original Message ------------




 
 Reply 
 
Phani
Phani
05:54 May-24-2005
Re: Phased array Probes
----------- Start Original Message -----------
: Because the sound field is steered or focused, as indicated in the previous response, the individual elements in the array must be designed properly so sound field will maintain its integrity over the intended phasing range. Older style linear arrays with large elements are not suitable for many phased applications. This is the reason many phased arrays appear smaller than non-phased designs.
: I hope this helps.
: Paul
: : The simple answer is yes they are the same, but not exactly. An array of any shape is 'phased' by driving the different array elements with different timing, so that the resultant beam is scanned, steered or focused.
: : Most phased array transducers are linear arrays, but annular, segmented or 2-D arrays can also be driven by phased array equipment
: : Joe
: :
: : ---------- Start Original Message -----------
: : : Can any Please tell me the difference between the Phase array transducers and linear array transducers.
: : : are they same or different?
: : : Thanks
: : : Phani
------------ End Original Message ------------

Thank you very much.

Regards
Phani


 
 Reply 
 

Product Spotlight

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Aerospace Systems - Automated Ultrasonic Inspection

USL are specialists in the design and manufacture of turnkey ultrasonic inspection systems for aer
...
ospace applications. From monolithic composites to complex honeycomb structures. This video shows just a few examples of what is possible, find out more at: www.ultrasonic-sciences.co.uk
>