Gharieb Adly Ali
Other, Ultrasonic Researcher
National Institute for Standards, Egypt, Joined Oct 1999, 1

Gharieb Adly Ali

Other, Ultrasonic Researcher
National Institute for Standards,
Egypt,
Joined Oct 1999
1
05:04 Sep-18-2000
Elect.Impedance of PZT Pickup


Dear colleagues

For economical purpose I had construct a simple PZT pickup
From PZT -4 Material of Fundamental frequency 2MHZ
When I measured the Electrical Impedance of Pickup against frequency
(Over frequency range 10 KHz to 4 MHZ )
I was found three Peaks
1- first at 250 kHz
2- second at 850 kHz
3- third at 3300 kHz
I Haven't explanation for this result, may be any colleague
has an explanation
Thank you very much



    
 
 
Jim Barshinger
Engineering
General Electric Global Research Center, USA, Joined Aug 2000, 8

Jim Barshinger

Engineering
General Electric Global Research Center,
USA,
Joined Aug 2000
8
05:44 Sep-18-2000
Re: Elect.Impedance of PZT Pickup
:
: Dear colleagues

: For economical purpose I had construct a simple PZT pickup
: From PZT -4 Material of Fundamental frequency 2MHZ
: When I measured the Electrical Impedance of Pickup against frequency
: (Over frequency range 10 KHz to 4 MHZ )
: I was found three Peaks
: 1- first at 250 kHz
: 2- second at 850 kHz
: 3- third at 3300 kHz
: I Haven't explanation for this result, may be any colleague
: has an explanation
: Thank you very much

The first and second peaks are most likely lateral resonances in the material. If you only have one lateral dimension, for instance a circular or square ceramic, I would guess that the 250 kHz peak is the fundamental lateral resonance and the 850 kHz peak is the third harmonic of the lateral resonance. The 3300 kHz peak should be your fundamental thickness mode resonance. I'm guessing that you are measuring the parallel resonance which will be a point of maximum real impedance. The series resonance should occur slightly lower in frequency and is a point of minimum real impedance. This should occur at 2 MHz (if you have ground your ceramic to the correct thickness). The center frequency that the device will run at depends on whether your recieving electronics matches better with the series or parallel resonance.

Good luck,
Jim





    
 
 

Product Spotlight

Teletest Focus+

Teletest Focus+ electronics have superior capabilities than rivals on the market. Beyond the usual
...
test features, Focus+ has 24 transmit channels and 24 receive channels, with an additional on-board switching capabilities. The instrument's frequency range is 10–300 kHz.
>

I&T Nardoni

NDT, RESEARCH AND DEVELOPMENT OF NEW METHODOLOGY, TRAINING CENTER I&T NARDON INSTITUTE was idiated
...
in 1988 by Giuseppe Nardoni, now president and owner of the company, based on his multi-annual and international experience in the field of NDT.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>