where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Volume Graphics GmbH
By choosing Volume Graphics software, you can rely on more than 20 years of experience in the development of software for non-destructive testi ...
2377 views
Career Discussions
Nigel Armstrong
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel Armstrong

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
09:42 Aug-04-2007
Vessel Fabrication Inspection Test Plan

I have been asked to produce a generic guide ITP to be supplied to fabricators of ASME VIII vessels. To prevent me reinventing the wheel does anyone have an electronic example (Excel preferably) theu could kindly provide me. You (or I) could remove all traces of point of origin. Please be assured I wont be goofing off playing golf on the time saved, my other rremit is for an ITP taking account of Russian standards requirements.

Please email me if you can help.

Thanks in advance.


 
 Reply 
 
Larry Mullins
Larry Mullins
06:44 Aug-08-2007
Re: Vessel Fabrication Inspection Test Plan
----------- Start Original Message -----------
: I have been asked to produce a generic guide ITP to be supplied to fabricators of ASME VIII vessels. To prevent me reinventing the wheel does anyone have an electronic example (Excel preferably) theu could kindly provide me. You (or I) could remove all traces of point of origin. Please be assured I wont be goofing off playing golf on the time saved, my other rremit is for an ITP taking account of Russian standards requirements.
: Please email me if you can help.
: Thanks in advance.
------------ End Original Message ------------

INSPECTION or EXAMINATION??? - very different things. Inspection is the activities of the AI and or Owner. Examination is the fabricator, and based on Code, TechSpec and QA program. Outlining the minimums of Code examination is easy. The rest is difficult and requires research. You are asking for trouble if you believe it is generic - you stand to miss alot of critical stuff.


 
 Reply 
 
tlang
tlang
08:19 Aug-08-2007
Re: Vessel Fabrication Inspection Test Plan
I have developed Quality programs and inspection test plans for pressure vessel systems before. The ITP program will have to be developed specifically to the activities of the AI and or Owner. As pointed out on the last message posted, the examination is specific to the fabricator based on Code, TechSpec and the QA program.


 
 Reply 
 
umarfaruk
umarfaruk
01:10 Aug-30-2007
Re: Vessel Fabrication Inspection Test Plan
----------- Start Original Message -----------
: I have developed Quality programs and inspection test plans for pressure vessel systems before. The ITP program will have to be developed specifically to the activities of the AI and or Owner. As pointed out on the last message posted, the examination is specific to the fabricator based on Code, TechSpec and the QA program.
------------ End Original Message ------------

can u send me the program im thankfull 2 u




 
 Reply 
 

Product Spotlight

Content on Demand by Eddyfi Technologies

Finding yourself in front of a screen practicing safe social distancing instead of out in the fiel
...
d? At Eddyfi Technologies, we are doing our part in helping you be better prepared for what comes next. We introduce to you Eddyfi on Demand. Fill your schedule with webinars, how-to videos, informative technical papers and our NEW addition: Eddyfi Academy. There, you will have access to FREE online courses and obtain certificates of attendance once completed in order for you to include these e-learning sessions in your log of required training hours. Join us today. Stay safe, stay Beyond Current.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window