Career Discussions
tomas perez a.
tomas perez a.
00:03 Jul-25-2007
vacuum box

Hi....everybody, could anybody help me? Where I can to get in USA, any company to buy vacuun box, to made "vacuum test in welds"?

I'd like to buy anyone.

Regards.


 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 159

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
159
07:23 Jul-25-2007
Re: vacuum box
----------- Start Original Message -----------
: Hi....everybody, could anybody help me? Where I can to get in USA, any company to buy vacuun box, to made "vacuum test in welds"?
: I'd like to buy anyone.
: Regards.
------------ End Original Message ------------

G'day Tomas,
Silverwing do a range of Vacuum boxes here is the link to their website for the US distributors, http://www.silverwinguk.com/en/agents/Americas/usa.htm

Regards
Neil


 
 Reply 
 
Floyd Atkinson
Floyd Atkinson
05:20 Dec-16-2007
Re: vacuum box
Tomas ,

Try,

http://www.alibaba.com/catalog/11910502/Vacuum_Box_For_Leak_Testing.html

Remember that your application will require a calibrated device to measure a minimum 10 PSI pressure.

Good luck.

----------- Start Original Message -----------
: Hi....everybody, could anybody help me? Where I can to get in USA, any company to buy vacuun box, to made "vacuum test in welds"?
: I'd like to buy anyone.
: Regards.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

AIS229 - Multipurpose Real Time System

Latest standard & automatic real time system developed by Balteau. The AIS229 has been designed to
...
do series inspection in a wide variety of industry. Composed of a shielded cabinet, 5 axis manipulator, x-ray generator and tubehead from 160kV to 225kV, a fl at panel & much more, the AIS229 is most certainly one of the most multipurpose RTR system available on the market.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>