01:08 Oct-24-2000
Ultrasonic tress meter

We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.



    
 
 
Pavel Pauliny (Rolf Diederichs)
Director
PP-Kontroltech, Slovak Republic, Joined Oct 2000, 1

Pavel Pauliny (Rolf Diederichs)

Director
PP-Kontroltech,
Slovak Republic,
Joined Oct 2000
1
02:20 Oct-24-2000
Re: Ultrasonic tress meter
Dear Forum Members,

it is important to enter without spelling errors your email address.
The Forum profile of Pavel Pauliny was registered with the email address "pauliny@ba.telekom.sk".
But in his first message Pavel Pauliny used "pauliny@ba.telecom.sk" as email address,
thus the database could not recognize the correct Forum profile.

Rolf Diederichs

-------------
: We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.




    
 
 
Dave Wilkes
Dave Wilkes
00:02 Oct-25-2000
Re: Ultrasonic tress meter



    
 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 295

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
295
07:23 Oct-26-2000
Re: Ultrasonic tress meter
: We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.

Hi.
We represent Quasar International Inc. in the United Kingdom (and through much of Europe).
Their RI-2000 instrument measures compressive Residual Stresses in many components, such as Bearing Elements, Turbine Disks, Railway Wheels etc.

They have also used this equipment sucessfully in detecting fatigue cracks in Railway Wheels.

Please email me for more information, or see our web pages.

Godfrey@hands-ndt.co.uk
www.hands-ndt.co.uk

Regards,

Godfrey Hands




    
 
 
Dave Utrata
R & D,
Center for NDE, Iowa State University, USA, Joined Feb 2000, 37

Dave Utrata

R & D,
Center for NDE, Iowa State University,
USA,
Joined Feb 2000
37
07:57 Oct-26-2000
Re: Ultrasonic tress meter
: We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.

The Fraunhofer Institute in Saarbrucken has developed a device based on UT to measure such stresses; if you contact them, give my reagrds to Eckhardt Schneider, the gentleman you should talk to on this matter.

The Polish Academy of Sciences also developed a device along similar principles, but it did not evolve into such a comprehensive package as the German device. However, I personally found this device quite useful and portable in my previous work. The gentleman to talk to there is Jacek Szelazek. Again, give my regards should you contact him.

I must also confess that the suggestion of using RI techniques, as suggested in another response posted here, truly surprises me. I am very suspicious of claims to determine residual stresses in railway wheels by this method, particularly keeping in mind the other changes, metallurgical and geometric, that wheels go through during service.

Regards,
Dave Utrata

p.s. here are two e-mail addresses for the gentlemen I indicated:

schneider@izfp.fhg.de
jszela@ippt.gov.pl


    
 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 605

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
605
09:52 Oct-26-2000
Re: Ultrasonic tress meter
Eckhardt Schneider is member of this forum, so he may listen our talks.
His profile provides a query to his 6 published articles currently on this server.
For example: Ultrasonic Evaluation of Stresses in the Rims of Railroad Wheels
http://www.ndt.net/article/ecndt98/rail/306/306.htm

Rolf Diederichs

-----------
: : We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.

: The Fraunhofer Institute in Saarbrucken has developed a device based on UT to measure such stresses; if you contact them, give my reagrds to Eckhardt Schneider, the gentleman you should talk to on this matter.

: The Polish Academy of Sciences also developed a device along similar principles, but it did not evolve into such a comprehensive package as the German device. However, I personally found this device quite useful and portable in my previous work. The gentleman to talk to there is Jacek Szelazek. Again, give my regards should you contact him.

: I must also confess that the suggestion of using RI techniques, as suggested in another response posted here, truly surprises me. I am very suspicious of claims to determine residual stresses in railway wheels by this method, particularly keeping in mind the other changes, metallurgical and geometric, that wheels go through during service.

: Regards,
: Dave Utrata

: p.s. here are two e-mail addresses for the gentlemen I indicated:

: schneider@izfp.fhg.de
: jszela@ippt.gov.pl




    
 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 295

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
295
08:26 Oct-27-2000
Re: Ultrasonic tress meter
: Eckhardt Schneider is member of this forum, so he may listen our talks.
: His profile provides a query to his 6 published articles currently on this server.
: For example: Ultrasonic Evaluation of Stresses in the Rims of Railroad Wheels
: http://www.ndt.net/article/ecndt98/rail/306/306.htm

: Rolf Diederichs

: -----------
: : : We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.

: : The Fraunhofer Institute in Saarbrucken has developed a device based on UT to measure such stresses; if you contact them, give my reagrds to Eckhardt Schneider, the gentleman you should talk to on this matter.

: : The Polish Academy of Sciences also developed a device along similar principles, but it did not evolve into such a comprehensive package as the German device. However, I personally found this device quite useful and portable in my previous work. The gentleman to talk to there is Jacek Szelazek. Again, give my regards should you contact him.

: : I must also confess that the suggestion of using RI techniques, as suggested in another response posted here, truly surprises me. I am very suspicious of claims to determine residual stresses in railway wheels by this method, particularly keeping in mind the other changes, metallurgical and geometric, that wheels go through during service.

: : Regards,
: : Dave Utrata

: : p.s. here are two e-mail addresses for the gentlemen I indicated:

: : schneider@izfp.fhg.de
: : jszela@ippt.gov.pl


Hi,
In reply to the surprise that Resonant Inspection can determine levels of residual stress in railroad wheels, I would like to add the following comments.

Normal Resonant Inspection, where the wheel is excited with a hammer (wheel tapping) will definitely be influenced by such factors as geometric and metallurgical changes.
The Quasar Resonant Inspection system uses the mathematical relationships between several different (modes of) resonances to compensate for these other changes.
This means that our measurements are largely not influenced by these otherwise interfering changes.
These methods are patented by Quasar.

Regards,

Godfrey Hands



    
 
 
Massimo Carminati
Consultant
procontrol, Italy, Joined Jul 2000, 6

Massimo Carminati

Consultant
procontrol,
Italy,
Joined Jul 2000
6
09:23 Oct-27-2000
Re: Ultrasonic tress meter
: We are looking for manufacture company for Ultrasonic tress meter for measurement of hoop residual stress in monoblock railway wheels.

I'm the Quasar Development Engineer for Italy and I would like to confirm Mr. Godfrey Hands suggestions, because I have had some promising results on these items too. About geometric variations during service, it is a very good argument, but, for example, the diameter reduction caused by wearing, will affect only the resonance frequencies related to the wheel race.

For more informations please contact also

Jim Schwarz Jim@quasarintl.com
Robert H. Nath Bob@quasarintl.com





    
 
 
Dave Utrata
R & D,
Center for NDE, Iowa State University, USA, Joined Feb 2000, 37

Dave Utrata

R & D,
Center for NDE, Iowa State University,
USA,
Joined Feb 2000
37
01:29 Nov-03-2000
Re: Ultrasonic tress meter
: Hi,
: In reply to the surprise that Resonant Inspection can determine levels of residual stress in railroad wheels, I would like to add the following comments.

: Normal Resonant Inspection, where the wheel is excited with a hammer (wheel tapping) will definitely be influenced by such factors as geometric and metallurgical changes.
: The Quasar Resonant Inspection system uses the mathematical relationships between several different (modes of) resonances to compensate for these other changes.
: This means that our measurements are largely not influenced by these otherwise interfering changes.
: These methods are patented by Quasar.

: Regards,

: Godfrey Hands


With all respect, I am still skeptical that resonant inspection could do much more than provide a go/no-go interpretation of (hoop) stress in railroad wheels. Previous work that I was involved with indicated that both surface readings and a bulk reading would be necessary to render a full picture of the state of stress in wheels. In such a manner, the bulk effects of a stress gradient could be weighed by how high of a stress was concentrated toward the front or rear rim face. The consequences of knowing how stress is distributred in a wheel rim is as important as knowing how much "total" hoop stress is present.



    
 
 
Arnulfo
Arnulfo
07:50 Dec-06-2006
Anton
5e6a9d3147aa


    
 
 

Product Spotlight

CIVA 2017 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window