Hi-Spec Systems
we are specialised in the design, development and manufacture of Phased Array and Time-of-Flight Diffraction (ToFD) ultrasonic inspection systems.
1844 views
Technical Discussions
David Hirsch
David Hirsch
00:06 Oct-29-2000
Concrete thickness testing, needs solution

The requirement is to measure the thickness of precast reinforced
concrete products, particularly concrete pipes and culverts before they
are installed i.e. in the factory yard or on the delivery site.

The product thickness can range from around 50 mm to 120 mm with easy
access to the external product surfaces but limited and difficult access to
the internal surface - as for example, in the case of a small diameter
pipe 2.5 m long.

Steel reinforcement content and pattern will vary with each product

Measurement accuracy desirably should be of the order of 2% but if
necessary up to 5% would be considered.

Portable battery operated equipment would be preferred, but is not
essential.

Products may have a thin plastic sheet lining over part of the internal
surface

Ideally the instrument should enable a thickness profile to be obtained
by traversing along the length of the product. If some form of
calibration is needed it would be possible to physically measure the
thickness at the beginning and end of such a traverse

Moisture content, cement content and degree of compaction of the concrete
may vary between products but should be consistent in each individual
product.

Obviously the radius of curvature of the external surface of a pipe is
dependent on the pipe diameter - a minimum external diameter of 750 mm is
envisaged.

If the above information is insufficient please advise what other information
is required.



 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:46 Oct-29-2000
Re: Concrete thickness testing, needs solution
Dear David,

The Lixi Profiler will measure both walls at the
same time with 2% repeatable accuracy. Your Email
address David Hirsch
came back as non deliverable.


 
 Reply 
 
William Friedman
R & D,
Lockheed Martin, USA, Joined Nov 1998, 6

William Friedman

R & D,
Lockheed Martin,
USA,
Joined Nov 1998
6
05:20 Nov-13-2000
Re: Concrete thickness testing, needs solution
: The requirement is to measure the thickness of precast reinforced
: concrete products, particularly concrete pipes and culverts before they
: are installed i.e. in the factory yard or on the delivery site.

I suggest you look at the Impact Echo technique which has been shown to
be effective at measuring the thickness of reinforced
concrete. Check the response in this forum by William
Streett on 12 May 1999 for more information and references.


 
 Reply 
 
Giuseppe Nardoni
Director
I&T Nardoni Institute, Italy, Joined Dec 1999, 4

Giuseppe Nardoni

Director
I&T Nardoni Institute,
Italy,
Joined Dec 1999
4
05:38 Nov-13-2000
Re: Concrete thickness testing, needs solution
In Roma in the exhibition of the 15 World Conference on NDT I have measured
with a potrable instrument from one side the thickness of a 450 mm wall of
the congress hall . The equpmenr works on radar waves principle .The
transducer is a box of 70 x 150 mm with 16 transducers .
For any othe information call me at 0039-348- 2280470 .

best regards
G:.NARDONI
Company : I&T Nardoni Institute

: The requirement is to measure the thickness of precast reinforced
: concrete products, particularly concrete pipes and culverts before they
: are installed i.e. in the factory yard or on the delivery site.

: The product thickness can range from around 50 mm to 120 mm with easy
: access to the external product surfaces but limited and difficult access to
: the internal surface - as for example, in the case of a small diameter
: pipe 2.5 m long.

: Steel reinforcement content and pattern will vary with each product

: Measurement accuracy desirably should be of the order of 2% but if
: necessary up to 5% would be considered.

: Portable battery operated equipment would be preferred, but is not
: essential.

: Products may have a thin plastic sheet lining over part of the internal
: surface

: Ideally the instrument should enable a thickness profile to be obtained
: by traversing along the length of the product. If some form of
: calibration is needed it would be possible to physically measure the
: thickness at the beginning and end of such a traverse

: Moisture content, cement content and degree of compaction of the concrete
: may vary between products but should be consistent in each individual
: product.

: Obviously the radius of curvature of the external surface of a pipe is
: dependent on the pipe diameter - a minimum external diameter of 750 mm is
: envisaged.

: If the above information is insufficient please advise what other information
: is required.




 
 Reply 
 
Otto Kroggel
Otto Kroggel
08:45 Dec-01-2000
Re: Concrete thickness testing, needs solution
: The requirement is to measure the thickness of precast reinforced
: concrete products, particularly concrete pipes and culverts before they
: are installed i.e. in the factory yard or on the delivery site.

: The product thickness can range from around 50 mm to 120 mm with easy
: access to the external product surfaces but limited and difficult access to
: the internal surface - as for example, in the case of a small diameter
: pipe 2.5 m long.

: Steel reinforcement content and pattern will vary with each product

: Measurement accuracy desirably should be of the order of 2% but if
: necessary up to 5% would be considered.

: Portable battery operated equipment would be preferred, but is not
: essential.

: Products may have a thin plastic sheet lining over part of the internal
: surface

: Ideally the instrument should enable a thickness profile to be obtained
: by traversing along the length of the product. If some form of
:calibration is needed it would be possible to physically measure the
: thickness at the beginning and end of such a traverse

: Moisture content, cement content and degree of compaction of the concrete
: may vary between products but should be consistent in each individual
: product.

: Obviously the radius of curvature of the external surface of a pipe is
: dependent on the pipe diameter - a minimum external diameter of 750 mm is
: envisaged.

: If the above information is insufficient please advise what other information
: is required.

Dear David,

I can offer an ultrasound equipment, which will solve your problem.
It uses a "dry" coupling and is therefore doesn´t have high requirements with respect to the evenness of the concrete surface.
A little bit of roughness is even better for the coupling
It takes about 1-2 seconds to take a measurement at a single point. the device is battery-operated and stores 960 single measurements in its local memory.
Thedata can easily be transferred from the local memory to a lap-top etc.
The data are represented on a small screen on the device itself in a way making it easy to interpret the results during the measurements and also to judge the concrete with respect to honeycombs etc.

I would not recommend to use Radar techniques, because of the unknown moisture situation in the concrete
Impact -echo application is limited to a certain minimum thickness because of the limitation of the maximum frequency generated by the " hammering mechanism".

Best regards Otto Kroggel


 
 Reply 
 
Dan E. Johnson
Dan E. Johnson
01:56 Dec-04-2000
Re: Concrete thickness testing, needs solution
: : The requirement is to measure the thickness of precast reinforced
: : concrete products, particularly concrete pipes and culverts before they
: : are installed i.e. in the factory yard or on the delivery site.
:
: I suggest you look at the Impact Echo technique which has been shown to
: be effective at measuring the thickness of reinforced
: concrete. Check the response in this forum by William
: Streett on 12 May 1999 for more information and references.

David,

I concur with the thoughts presented above regarding Impact Echo testing, as it is an effective measuring tool for reinforced concrete of depths within the thivkness range you require. More information on this technique can be found at www.impactecho.com, including information about the book "Impact Echo - Nondestructive Evaluation of Concrete and Masonry" written by William Streett and Mary Sansalone.


 
 Reply 
 
arun sankhat
arun sankhat
05:33 Jul-30-2002
Re: Concrete thickness testing, needs solution
sir,
i would like to know more about the method and how to analyse the stress waves that are reflected back from any discontinuity.
arun

: : : The requirement is to measure the thickness of precast reinforced
: : : concrete products, particularly concrete pipes and culverts before they
: : : are installed i.e. in the factory yard or on the delivery site.
: :
: : I suggest you look at the Impact Echo technique which has been shown to
: : be effective at measuring the thickness of reinforced
: : concrete. Check the response in this forum by William
: : Streett on 12 May 1999 for more information and references.

: David,

: I concur with the thoughts presented above regarding Impact Echo testing, as it is an effective measuring tool for reinforced concrete of depths within the thivkness range you require. More information on this technique can be found at www.impactecho.com, including information about the book "Impact Echo - Nondestructive Evaluation of Concrete and Masonry" written by William Streett and Mary Sansalone.




 
 Reply 
 

Product Spotlight

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window