Career Discussions
Filipe Matta
NDT Inspector
ITG, Portugal, Joined Nov 2008, 2

Filipe Matta

NDT Inspector
ITG,
Portugal,
Joined Nov 2008
2
06:12 Nov-05-2008
EMAT

I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
Can someone give me information on companies who provide EMAT devices that fulfill my needs?
Thanks
Filipe


 
 Reply 
 
Steve
Consultant, Advanced NDT Services
Advanced Integrity Solutions, USA, Joined Oct 2008, 1

Steve

Consultant, Advanced NDT Services
Advanced Integrity Solutions,
USA,
Joined Oct 2008
1
08:40 Nov-05-2008
Re: EMAT
Call Mark Adams at Spectrum Sales and Services

e-mail: markemat@aol.com

He has been in the business for over 10 years and is a wealth of knowledge.

Steve
----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------




 
 Reply 
 
Ron Alers
Director, - - President of EMAT Ultrasonics Inc.
USA, Joined Feb 2007, 4

Ron Alers

Director, - - President of EMAT Ultrasonics Inc.
USA,
Joined Feb 2007
4
00:16 Nov-07-2008
Re: EMAT
Dear Filipe,
Sonic Sensors of EMAT Ultrasonics Inc. has numerous industrial field service tools specifically designed for vessels, tanks, and piping. Please contact us at the numbers below and we can discuss all the possibilities. We have equipment for sale, license, or field service companies which can provide the service for you.

Cordially,
Ron Alers
----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------




 
 Reply 
 
Frank Passarelli
President
USA, Joined Jun 2005, 1

Frank Passarelli

President
USA,
Joined Jun 2005
1
01:39 Nov-07-2008
Re: EMAT
----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------

Filipe,

Resonic is a manufacturer of The ARIS line of EMAT based EMAR type systems. We can provide spot check as well as permanent sensor installations for such applications


 
 Reply 
 
Larry Hopper
Larry Hopper
04:32 Nov-07-2008
Re: EMAT
----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------

There is another alternative that is very effective. The alternative is Low Frequency Electromagnetics. This is used all over the world for tank wall scanning. Secondly, Balanced field eddy current is available for weld crack inspections. Contact TesTex for more information.


 
 Reply 
 
Joe Buckley
Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT, United Kingdom, Joined Oct 1999, 528

Joe Buckley

Consultant, ASNT L-III, Honorary Secretary of BINDT
Level X NDT, BINDT,
United Kingdom,
Joined Oct 1999
528
06:32 Nov-07-2008
Re: EMAT
At the risk of being a bit mundane, are you sure you need to use the exotic methods?

If you want to carry out wall thickness reduction surveys and weld depth integrity checking on pressure vessels then "conventional" gel/water coupled ultrasonics (whether with monoelement transducers, Phased array or AUT) is well accepted and code approved. EMAT and low frequency ET may work, but you will be off in a minefield of performance demonstation, limited availability of trained operators etc. I would recommed that you be certain you need to use these methods before you go down that route.

For weld cracking (as against problems at depth) then conventional Eddy current weld inspection or ACFM may be worth considering.

Rgds

Joe


----------- Start Original Message -----------
: : I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: : Cansomeone give me information on companies who provide EMAT devices that fulfill my needs?
: : Thanks
: : Filipe
: There is another alternative that is very effective. The alternative is Low Frequency Electromagnetics. This is used all over the world for tank wall scanning. Secondly, Balanced field eddy current is available for weld crack inspections. Contact TesTex for more information.
------------ End Original Message ------------




 
 Reply 
 
Mark Potter
Mark Potter
03:11 Nov-09-2008
Re: EMAT
Dear Filipe,

we make EMAT based inspection systems - if the pressure vessels are steel, we have an off-the-shelf system that should be suitable for wall thinning, and can make weld inspection EMAT systems bespoke.

Sincerely,

Mark

----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>