We have been asked to perform UT inspection of pipelines held by a rack at some meters of height.
Does anyone know which method can be employed and if there is a company performing this kind of inspection ?

Thanks.

Amedeo.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:06 Nov-27-2000
Inspection of Pipelines on rack
The Profiler is being used in Australia to measure the total pipe wall thickness and support beam thickness.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:07 Nov-27-2000
Inspection of Pipelines on rack
The Lixi Profiler is being used in Australia to measure the total pipe wall thickness and support beam thickness.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:07 Nov-27-2000
Inspection of Pipelines on rack
The Lixi Profiler is being used in Australia to measure the total pipe wall thickness and support beam thickness.


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
04:36 Nov-28-2000
Re: inspection of Pipelines on rack
One of the ways to do screening is to use Guided Wave Ultrasonics. If the pipe is uninsulated you can screen considerable distances from one access point onto the pipe.

We can assist you with this.

Please feel free to contact me for more details

John O'Brien
obirc@aol.com



 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
06:40 Nov-28-2000
Re: inspection of Pipelines on rack
More details of the task needed, really. But for UT of the welds, local corrosion and HIC mapping you could use an automated UT system.

Some P-scan UT info available at ...
http://www.inspection.co.uk/p-scan
http://www.p-scan.com



 
 Reply 
 
mohammad mosa shabanian
mohammad mosa shabanian
01:21 Dec-02-2000
Re: inspection of Pipelines on rack
: More details of the task needed, really. But for UT of the welds, local corrosion and HIC mapping you could use an automated UT system.

: Some P-scan UT info available at ...
: http://www.inspection.co.uk/p-scan
: http://www.p-scan.com




 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Research and Applications Development For NDT

The Research and Applications Development (RAD) group is a newly formed team within Acuren dedicat
...
ed to tackling challenging inspection problems. Our focus is the development of novel, field deployable, advanced inspection techniques for use in cases where standard NDT methods are ineffective. We don't wait for new innovations, we engineer them. From concept to commissioning.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window