inspection of Pipelines on rack

We have been asked to perform UT inspection of pipelines held by a rack at some meters of height.
Does anyone know which method can be employed and if there is a company performing this kind of inspection ?

Thanks.

Amedeo.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:06 Nov-27-2000
Inspection of Pipelines on rack
The Profiler is being used in Australia to measure the total pipe wall thickness and support beam thickness.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:07 Nov-27-2000
Inspection of Pipelines on rack
The Lixi Profiler is being used in Australia to measure the total pipe wall thickness and support beam thickness.


 
 Reply 
 
Joseph Pascente
Engineering
Lixi, Inc., USA, Joined Nov 1998, 39

Joseph Pascente

Engineering
Lixi, Inc.,
USA,
Joined Nov 1998
39
05:07 Nov-27-2000
Inspection of Pipelines on rack
The Lixi Profiler is being used in Australia to measure the total pipe wall thickness and support beam thickness.


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
04:36 Nov-28-2000
Re: inspection of Pipelines on rack
One of the ways to do screening is to use Guided Wave Ultrasonics. If the pipe is uninsulated you can screen considerable distances from one access point onto the pipe.

We can assist you with this.

Please feel free to contact me for more details

John O'Brien
obirc@aol.com



 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
06:40 Nov-28-2000
Re: inspection of Pipelines on rack
More details of the task needed, really. But for UT of the welds, local corrosion and HIC mapping you could use an automated UT system.

Some P-scan UT info available at ...
http://www.inspection.co.uk/p-scan
http://www.p-scan.com



 
 Reply 
 
mohammad mosa shabanian
mohammad mosa shabanian
01:21 Dec-02-2000
Re: inspection of Pipelines on rack
: More details of the task needed, really. But for UT of the welds, local corrosion and HIC mapping you could use an automated UT system.

: Some P-scan UT info available at ...
: http://www.inspection.co.uk/p-scan
: http://www.p-scan.com




 
 Reply 
 

Product Spotlight

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window