Nick Welland
Nick Welland
09:09 Dec-05-2000
Positive Material Identification

I am looking for suppliers of equipment for positive material identification of metals, principally stainless steels.
Instrumentation could be XRF or OES; must be portable and economical.
Regards
Nick Welland


 
 Reply 
 
Guido Crapels
Guido Crapels
09:20 Dec-05-2000
Re: Positive Material Identification



 
 Reply 
 
Guido Crapels
Guido Crapels
01:15 Dec-05-2000
Re: Positive Material Identification



 
 Reply 
 
Peter Faulkner
Peter Faulkner
03:06 May-01-2001
Re: Positive Material Identification
: I am looking for suppliers of equipment for positive material identification of metals, principally stainless steels.
: Instrumentation could be XRF or OES; must be portable and economical.
: Regards
: Nick Welland

Have you been successful with your search yet?
WE at Niton UK can offer both XRF and OES usually ex demo units available periodically
Peter Faulkner


 
 Reply 
 
p.saniee
p.saniee
09:34 Jul-18-2001
Re: Positive Material Identification
: : I am looking for suppliers of equipment for positive material identification of metals, principally stainless steels.

best regards
saniee


 
 Reply 
 

Product Spotlight

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

GUL QSR1® Scanning

How do you measure pipe wall thickness without direct access to the area? QSR® Scanning - Guide Wav
...
e Quantitative Short Range Scanning.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window