M. W. Moyer
M. W. Moyer
06:34 Feb-19-2001
Radial Surface Waves

Does anyone have some references about using radial surface waves
from short focused transducers to detect surface and near surface
defects and material property variations?
Thanks in advance for your help.

M. W. Moyer


 
 Reply 
 
Albrecht Maurer
Albrecht Maurer
08:48 Feb-20-2001
Re: Radial Surface Waves
: Does anyone have some references about using radial surface waves
: from short focused transducers to detect surface and near surface
: defects and material property variations?
: Thanks in advance for your help.
.
: M. W. Moyer
.
Mr. Sebastian Gripp of our organisation has realized an industrial solution for surface testing of contoured turbine discs applying a specific rayleigh wave probe. The corresponding paper has been presented at the WCNDT in Rome last fall.


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
00:47 Feb-20-2001
Re: Radial Surface Waves
Mr Gripp's paper is available at:
Surface Crack Detection Using Rayleigh Waves - in immersion: A Novel Application of a Known Principle
http://www.ndt.net/article/wcndt00/papers/idn031/idn031.htm

Also I would like to take the opportunity to introduce a problem of the email address used in the forum message.
Albrecht Maurer used in his message the email address "albrecht_maurer@nukem.de",
but his Member Profile is registers with the email address "Nutronik@Nukem.de".
The system can set Profile and Exhibitors links only according to the registered Forum Profiles.

Mr. Maurer's Profile: http://www.ndt.net/wshop/profile/profiles/123.htm
NUKEM Nutronik GmbH: http://www.ndt.net/exhibit/stand/15_ky.htm

That means you shall use for forum messages always the email address of the profile.

Best regards
Rolf Diederichs

: : Does anyone have some references about using radial surface waves
: : from short focused transducers to detect surface and near surface
: : defects and material property variations?
: : Thanks in advance for your help.
: .
: : M. W. Moyer
: .
: Mr. Sebastian Gripp of our organisation has realized an industrial solution for surface testing of contoured turbine discs applying a specific rayleigh wave probe. The corresponding paper has been presented at the WCNDT in Rome last fall.
.



 
 Reply 
 
Albrecht Maurer
Engineering
GE Inspection Technologies, Germany, Joined Nov 1998, 1

Albrecht Maurer

Engineering
GE Inspection Technologies,
Germany,
Joined Nov 1998
1
00:55 Feb-20-2001
Re: Radial Surface Waves
(repeated message with the profile email address, by Rolf Diederichs)

Mr. Sebastian Gripp of our organisation has realized an industrial solution for surface testing of contoured turbine discs applying a specific rayleigh wave probe. The corresponding paper has been presented at the WCNDT in Rome last fall.

: Does anyone have some references about using radial surface waves
: from short focused transducers to detect surface and near surface
: defects and material property variations?
: Thanks in advance for your help.
.
: M. W. Moyer
.



 
 Reply 
 
Dr. Patel
Dr. Patel
03:16 May-02-2001
Re: Radial Surface Waves
: Does anyone have some references about using radial surface waves
: from short focused transducers to detect surface and near surface
: defects and material property variations?
: Thanks in advance for your help.
.
: M. W. Moyer
.I hope this will clarify the points. For past 3 years we are working on developing sensors and system for surface and subsurface characterization of materials in terms of surface velocities and amplitude information and we have a success. We have full facility at University which one can take advantage. The University is McMaster in Hamilton, Ontario or at Fallon Ultrasonics Inc in Hamilton.

Regards

Dr. Patel



 
 Reply 
 

Product Spotlight

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>