Technical Discussions
M. W. Moyer
M. W. Moyer
06:34 Feb-19-2001
Radial Surface Waves

Does anyone have some references about using radial surface waves
from short focused transducers to detect surface and near surface
defects and material property variations?
Thanks in advance for your help.

M. W. Moyer


 
 Reply 
 
Albrecht Maurer
Albrecht Maurer
08:48 Feb-20-2001
Re: Radial Surface Waves
: Does anyone have some references about using radial surface waves
: from short focused transducers to detect surface and near surface
: defects and material property variations?
: Thanks in advance for your help.
.
: M. W. Moyer
.
Mr. Sebastian Gripp of our organisation has realized an industrial solution for surface testing of contoured turbine discs applying a specific rayleigh wave probe. The corresponding paper has been presented at the WCNDT in Rome last fall.


 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 609

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
609
00:47 Feb-20-2001
Re: Radial Surface Waves
Mr Gripp's paper is available at:
Surface Crack Detection Using Rayleigh Waves - in immersion: A Novel Application of a Known Principle
http://www.ndt.net/article/wcndt00/papers/idn031/idn031.htm

Also I would like to take the opportunity to introduce a problem of the email address used in the forum message.
Albrecht Maurer used in his message the email address "albrecht_maurer@nukem.de",
but his Member Profile is registers with the email address "Nutronik@Nukem.de".
The system can set Profile and Exhibitors links only according to the registered Forum Profiles.

Mr. Maurer's Profile: http://www.ndt.net/wshop/profile/profiles/123.htm
NUKEM Nutronik GmbH: http://www.ndt.net/exhibit/stand/15_ky.htm

That means you shall use for forum messages always the email address of the profile.

Best regards
Rolf Diederichs

: : Does anyone have some references about using radial surface waves
: : from short focused transducers to detect surface and near surface
: : defects and material property variations?
: : Thanks in advance for your help.
: .
: : M. W. Moyer
: .
: Mr. Sebastian Gripp of our organisation has realized an industrial solution for surface testing of contoured turbine discs applying a specific rayleigh wave probe. The corresponding paper has been presented at the WCNDT in Rome last fall.
.



 
 Reply 
 
Albrecht Maurer
Engineering
GE Inspection Technologies, Germany, Joined Nov 1998, 1

Albrecht Maurer

Engineering
GE Inspection Technologies,
Germany,
Joined Nov 1998
1
00:55 Feb-20-2001
Re: Radial Surface Waves
(repeated message with the profile email address, by Rolf Diederichs)

Mr. Sebastian Gripp of our organisation has realized an industrial solution for surface testing of contoured turbine discs applying a specific rayleigh wave probe. The corresponding paper has been presented at the WCNDT in Rome last fall.

: Does anyone have some references about using radial surface waves
: from short focused transducers to detect surface and near surface
: defects and material property variations?
: Thanks in advance for your help.
.
: M. W. Moyer
.



 
 Reply 
 
Dr. Patel
Dr. Patel
03:16 May-02-2001
Re: Radial Surface Waves
: Does anyone have some references about using radial surface waves
: from short focused transducers to detect surface and near surface
: defects and material property variations?
: Thanks in advance for your help.
.
: M. W. Moyer
.I hope this will clarify the points. For past 3 years we are working on developing sensors and system for surface and subsurface characterization of materials in terms of surface velocities and amplitude information and we have a success. We have full facility at University which one can take advantage. The University is McMaster in Hamilton, Ontario or at Fallon Ultrasonics Inc in Hamilton.

Regards

Dr. Patel



 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

NovaScope 6000

The all-digital Novascope 6000 is a portable, ultra-high precision thickness gauge for high-speed
...
thickness measurement. Novascope 6000 has unmatched capabilities and unique features including: •Superior Resolution with high contrast, high-speed color RF display •High pulser voltage •Real-time video output •Increased internal/external data storage •Programmable SetUp features •Battery & AC Powered
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>