Vasco Teixeira
R & D, coatings production and inspection, stress analysi
University of Minho - Physics Centre, Portugal, Joined Feb 2000, 3

Vasco Teixeira

R & D, coatings production and inspection, stress analysi
University of Minho - Physics Centre,
Portugal,
Joined Feb 2000
3
08:53 Feb-26-2001
elastic parameters and quality control of PVD thin films

Dear colleagues,

I would like to know (and share some informations)concerning the amount of money involved in industry/ R&D institutes(europe and USA) to :
develop NDT systems for quality inspection of sputtered and physically vacuum deposited thin films for optical, microelectronic and mechanical industry.
and, for speciall systems to control residual stresses and elastic properties of as-deposited thin films and coatings on components in on-line coating production.

Thanks for any help

All the best

Vasco

vasco@fisica.uminho.pt
fax: +351 253 678 981
phone: +351 253 604334/20



 
 Reply 
 
Dr. Patel ND
Dr. Patel ND
01:41 May-02-2001
Re: elastic parameters and quality control of PVD thin films
: Dear colleagues,
.
: I would like to know (and share some informations)concerning the amount of money involved in industry/ R&D institutes(europe and USA) to :
: develop NDT systems for quality inspection of sputtered and physically vacuum deposited thin films for optical, microelectronic and mechanical industry.
: and, for speciall systems to control residual stresses and elastic properties of as-deposited thin films and coatings on components in on-line coating production.
.
: Thanks for any help
.
: All the best
.
: Vasco
.
: vasco@fisica.uminho.pt
: fax: +351 253 678 981
: phone: +351 253 604334/20
.
We are measuring stress in situ on metal and metal alloys and perhaps if you can send us more information on substrate and film thickness and what magnitude of stresses are imposed than we can help you as we have our own ultrasonic system which can measure stresses on thin materials.

Regards

Dr.Patel


 
 Reply 
 
Colin Nicolson
Colin Nicolson
05:34 Jul-04-2001
Re: elastic parameters and quality control of PVD thin films
A good method to control sputtered stress if use a substrate bias. This will tune the amount of gas incorporated into the film. Stress can be changed from tensile to compressive by varying the bias.

Sputter systems are commercially available for this type of applications. Papers and information of potential metals and there properties are hard to come by.

Colin Nicolson.
Process Engineer
Kymata Ltd.



 
 Reply 
 

Product Spotlight

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

iProbe - USB Phased Array Probe

Turn your PC, Laptop or Tablet into a powerful 32:64 Phased Array system with our USB powered Phas
...
ed Array iProbe and inspection software package. Perform affordable weld inspection and corrosion mapping inspections with this powerful but small system. The probe has a 100V pulser, 8K PRF, dual axis encoder input and achieves outstanding signal quality.
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window