Doug Irish
Doug Irish
08:33 Mar-12-2001
Ultrasonic testing of concrete

I am trying to determine if the Krautkramer USN 60 will test for voids, caused by erosion, in the underlayment of a large concrete floor.Thanks


 
 Reply 
 
Jim Sabol
Jim Sabol
08:28 Mar-13-2001
Re: Ultrasonic testing of concrete
: I am trying to determine if the Krautkramer USN 60 will test for voids, caused by erosion, in the underlayment of a large concrete floor.Thanks
. The USN 60 is not designed for this application. The frequency bandwidth is not low enough to ensure penetration of the concrete. More importantly, there is a basic limitation caused by the principles of ultrasonics. The interface between the bottom of the concrete and the underlayment will always appear as an air gap whether the underlayment is intact or missing because of erosion. We suggest ground penetrating radar as a better solution.



 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 280

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
280
01:43 Mar-23-2001
Re: Ultrasonic testing of concrete
UT is not the best solution for this. Try looking at Impact Echo device which is tailor made for this application. Try searching for Impact Echo or go to www.pacuk.co.uk


 
 Reply 
 
Michael Berke
Michael Berke
01:51 Mar-28-2001
Re: Ultrasonic testing of concrete
: I am trying to determine if the Krautkramer USN 60 will test for voids, caused by erosion, in the underlayment of a large concrete floor.Thanks
.I suggest to try with KRAUTKRAMER USM 23LF, a high power (1200 Volts), low frequency (50 - 500 kHz)Ultrasonic Flaw Detector, specially designed for high attenuative or coarse grain material. M. Berke, Krautkramer - Germany



 
 Reply 
 
Dan Johnson
Dan Johnson
05:46 Mar-28-2001
Re: Ultrasonic testing of concrete
: : I am trying to determine if the Krautkramer USN 60 will test for voids, caused by erosion, in the underlayment of a large concrete floor.Thanks

I suggest trying IMPACT ECHO TESTING, which works in the 1-60 kHz range, uses spherical impactors, and has been used in previous applications to determine the locations of such voids. This method corresponds to ASTM Standard C-1383-98 for measuring plate thickness. Dan E. Johnson, Physical Acoustics Corp., Princeton, NJ


 
 Reply 
 
oak
oak
02:40 Aug-29-2002
Re: Ultrasonic testing of concrete
: I am trying to determine if the Krautkramer USN 60 will test for voids, caused by erosion, in the underlayment of a large concrete floor.Thanks
.i want testing by ultrasonics of concreat


 
 Reply 
 
oak
oak
02:45 Aug-29-2002
Re: Ultrasonic testing of concrete
: : : I am trying to determine if the Krautkramer USN 60 will test for voids, caused by erosion, in the underlayment of a large concrete floor.Thanks
.
: I suggest trying IMPACT ECHO TESTING, which works in the 1-60 kHz range, uses spherical impactors, and has been used in previous applications to determine the locations of such voids. This method corresponds to ASTM Standard C-1383-98 for measuring plate thickness. Dan E. Johnson, Physical Acoustics Corp., Princeton, NJ
.testing of concreat



 
 Reply 
 
Melissa Rubio
Melissa Rubio
08:23 Sep-09-2002
Re: Ultrasonic testing of concrete
I would like to know if anyne has used Matlab to form artificial neural networks to test flaws in concrete non destructively.
please if anyone can help please do


 
 Reply 
 
Naveen Nair
Engineering
Indian Institute of Technology Madras, India, Joined Sep 2002, 1

Naveen Nair

Engineering
Indian Institute of Technology Madras,
India,
Joined Sep 2002
1
09:12 Sep-09-2002
Re: Ultrasonic testing of concrete
: I would like to know if anyne has used Matlab to form artificial neural networks to test flaws in concrete non destructively.
: please if anyone can help please do
.

Yes it can be done. I have used MATLAB based and self developed code to do NDE of certain composites. I have not specifically worked on concrete, but I am assuming that composites is a good enough generalisation.
please do let me know if i can be of any help
Nair




 
 Reply 
 
Apostolos Tsimogiannis
Engineering, and R&D and NDT Inspector
ENVIROCOUSTICS SA, Greece, Joined Jan 2000, 2

Apostolos Tsimogiannis

Engineering, and R&D and NDT Inspector
ENVIROCOUSTICS SA,
Greece,
Joined Jan 2000
2
00:13 Sep-18-2002
Re: Ultrasonic testing of concrete
: : I would like to know if anyne has used Matlab to form artificial neural networks to test flaws in concrete non destructively.
: : please if anyone can help please do
: .
.

We have done research work for both crack-like flaw detection, sizing and properties characterization, both in building (affected from earthquakes etc) and on laboratory specimens (during hardening and compression tests). The techniques we used were Acoustic Emission, Acousto-Ultrasonics and Ultrasonic velocity.
For signal discrimination we used Noesis a software for data analysis with Pattern Recognition and Neural Networks.
You can read about this work in published papers.
for example :

WCNDT 2000 ROME : Damage Level Evaluation and Characterization by Acoustic Emission and Acousto-Ultrasonics in Concrete Under Compressive Loads ( http://www.ndt.net/article/wcndt00/papers/idn449/idn449.htm)

ECNDT 2002 BARCELONA : DETERMINATION OF CONCRETE STRENGTH AND WATER TO CEMENT RATIO BY USING PATTERN RECOGNITION TECHNIQUES ON ACOUSTO-ULTRASONIC SIGNALS

See also the links.

best regards

Apostolos Tsimogiannis



 
 Reply 
 

Product Spotlight

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

YXLON Cougar EVO

Scalable small footprint X-ray inspection systems for assembly and laboratory applications. The
...
YXLON Cougar EVO series was designed to provide the "best-in- class" inspection solutions for SMT, semiconductor, and laboratory assembly applications, while maintaining a small system footprint for maximum convenience. With optimized software and hardware, these systems produce higher quality and more consistent results than other electronics inspection systems currently on the market.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window