Simulating Corrosion

We are going to start a program in which we need to test for ways to measure corroded and very rough surfaces. My question is if anyone knows how to corrode a surface so that is uneven, and not just creating a thinner sample?


 
 Reply 
 
Phil Herman Jr.
Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards, USA, Joined Oct 1999, 79

Phil Herman Jr.

Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards,
USA,
Joined Oct 1999
79
07:48 Apr-02-2001
Re: Simulating Corrosion
Justin,
PH Tool Reference Standards has developed a proprietary method to artificially recreate actual corrosion using the Electrical Discharge Machining (EDM) process. Corroded "pads" can faithfully simulate real corrosion while maintaining precise depth dimensions. Contact me if you need more info.

: We are going to start a program in which we need to test for ways to measure corroded and very rough surfaces. My question is if anyone knows how to corrode a surface so that is uneven, and not just creating a thinner sample?
.



 
 Reply 
 

Product Spotlight

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window