X Ray for 2" thickness pipeline

our next project is 2" thickness offshore pipeline , we need to applly ndt to the welds , shall X Ray be able to inspect the welds or we need another method , i have J.M.E crawler .



    
 
 
Guido Crapels
Guido Crapels
09:47 Apr-27-2001
Re: X Ray for 2" thickness pipeline
: our next project is 2" thickness offshore pipeline , we need to applly ndt to the welds , shall X Ray be able to inspect the welds or we need another method , i have J.M.E crawler .
.
Reply:

For this kind of thicknesses x-ray is not suitable. Conventional x-ray tubes cannot produce energies sufficiently high for useful radiographies of welding defects (theoretically, a linear accelerator could do the job, but will not fit onto a crawler and is way too large and expensive to be handled outside any dedicated facility). You would need something like a Co60 source, but this is not suitable regarding safety. The conventional Ir192 source (with lower energy) could theoretically meet the testing quality requirements (maybe), but would take a rather long exposure time and is therefore unlikely to be economical.
Even if you could qualify a radiography test in this case, the weld will comprise many layers in which small flaws can hide that will not be detected by radiography.
In most cases these kind of welds are examined by means of ultrasonics, like the RTD Rotoscan system. It is fast and produces the information required for proper testing for flaws like slag inclusions, lack of fusions and root flaws. The pulse-echo mode can be combined with Time of Flight testing in the same run. This technique is qualified for all major Pressure codes, on- and offshore likewise.



    
 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
09:40 Apr-27-2001
Re: X Ray for 2" thickness pipeline
: our next project is 2" thickness offshore pipeline , we need to applly ndt to the welds , shall X Ray be able to inspect the welds or we need another method , i have J.M.E crawler .
.
Wall thickness of 2" is very substantial. If this is
the real thickness then automated UT will be cheaper,
faster, more sensitive, and safer than any X-Ray
or Gamma-Ray crawler.

Take a look at http://www.inspection.co.uk or
http://www.force.dk for info on 'P_scan System 4'
and 'P-scan 4 Lite' systems.

Remember that you'll need fully trained and
experienced technicians to get the best out of any
automated UT system.


    
 
 
Massimo Carminati
Massimo Carminati
07:10 Apr-28-2001
Re: X Ray for 2" thickness pipeline
You can also check on the R/D Tech web site and look for more information on the Phased Array Pipe Wizard system. It is the most advanced system available fpr automated UT and the use of Phased Arrays may reduce the number of probes (in this case) by a factor of 10!


    
 
 
rajeev chaudhari
NDT Inspector
offshore testing & inspection services (I) pvt ltd, India, Joined Dec 2000, 17

rajeev chaudhari

NDT Inspector
offshore testing & inspection services (I) pvt ltd,
India,
Joined Dec 2000
17
02:20 Apr-28-2001
Re: X Ray for 2" thickness offshore pipeline
OTISLAB has complete facilities for NDT testing for various requirements. If you could let us know ID, OD, it will be easy to decide extact technique and equipment cababilities. We hope you will understand implication of incorrect details.





    
 
 
ender keskin
ender keskin
06:30 May-30-2001
x-ray apparatus for pipeline(up to 1" pipeline)
we are looking for x-ray apparatus for 14mm-16mm pipeline(meat thickness)
could you inform us where and which brand are we going to search?
could you give some e-mails,adresses,tels or any other connections?
we want to buy one asap.

best regards,

ender keskin


    
 
 
ender keskin
ender keskin
06:35 May-30-2001
pipeline
we are looking for grounding conducter,welder protctive tent,insulation detecting device,pipe bending machine and boring machine.
pls contact with us asap..

best regards,

ender keskin


    
 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window